Methods for enhancing the preservation of cellulosic materials and cellulosic materials prepared thereby
AssigneeAmerican Chemet Corporation
InventorDaniel Brimhall
Life of this patent
Estimating the term…
Abstract
Methods for treating cellulosic materials comprising introducing a liquid treating composition into the cellulosic material, the treating composition comprising a solution prepared from at least: (i) one or more of a copper amine complex or copper ammine complex, such as copper tetraamine carbonate, (ii) one or more of ammonia or a water-soluble amine and (iii) water; and exposing the cellulosic material provided thereby to carbon dioxide and/or carbonic acid to provide treated cellulosic material, and treated cellulosic materials prepared thereby.
Claims16
-76. (canceled)
Treated refractory softwood comprising
- refractory softwood, and
- a copper-containing compound formed in situ within the refractory softwood by exposing an aqueous solution of a copper ammine complex to one or more of carbon dioxide and carbonic acid,
- wherein the copper-containing compound penetrates at least about 80% of the treated refractory softwood as determined using AWPA Standard A72, and
- wherein the leaching of sectioned treated refractory softwood after 14 days as determined using AWPA Standard E11 is less than 25% of the total copper present in the sectioned treated refractory softwood.
The treated refractory softwood according to claim 1, wherein the treated refractory softwood further comprises a zinc-containing compound.
The treated refractory softwood according to claim 1, wherein the refractory softwood is Douglas Fir.
The treated refractory softwood according to claim 1, wherein the refractory softwood is Hem Fir.
The treated refractory softwood according to claim 1, wherein the refractory softwood is Spruce-Pine-Fir.
The treated refractory softwood according to claim 1, wherein the refractory softwood is Red Pie.
The treated refractory softwood according to claim 1, wherein the refractory softwood is Jack Pine.
The treated refractory softwood according to claim 1, wherein the treated refractory softwood comprises about 0.01 to about 0.5 lbs/ft3 of copper as determined using AWPA Standard A9.
The treated refractory softwood according to claim 8, wherein the treated refractory softwood comprises about 0.06 to about 0.15 lbs/ft3 of copper as determined using AWPA Standard A9.
The treated refractory softwood according to claim 8, wherein the treated refractory softwood comprises about 0.1 to about 0.35 lbs/ft3 of copper as determined using AWPA Standard A9.
The treated refractory softwood according to claim 1, wherein the treated refractory softwood is a dimensioned wood product.
The treated refractory softwood according to claim 8, wherein the treated refractory softwood is a dimensioned wood product.
The treated refractory softwood according to claim 9, wherein the treated refractory softwood is a dimensioned wood product.
The treated refractory softwood according to claim 10, wherein the treated refractory softwood is a dimensioned wood product.
The treated refractory softwood according to claim 1, wherein the copper-containing compound penetrates at least about 90% of the treated refractory softwood as determined using AWPA Standard A72.
Dependencies are inferred from the claim text.