Sanitary equipment part
AssigneeToto Ltd.
InventorsYuya SUZUKI, Saori UKIGAI, Hironori HATONO, Atsushi TERAMOTO, Yuichi TAKAMATSU, Hana ISHII
Life of this patent
Estimating the term…
Abstract
A part includes a base material, a colored layer, an intermediate layer, and a water-repellent-surface layer. The colored layer contains 35 at % to 99 at % of C, 0 at % to less than 40 at % of Cr, 0 at % to less than 15 at % of N, and more than 0 at % to less than 15 at % of O. The intermediate layer contains at least one metal atom selected from Cr, Zr, and Si; and an oxygen atom. The intermediate layer exhibits a sputtering time of 0.5 minutes or more to 9 minutes or less
Claims17
A part comprising at least a base material, a colored layer on the base material, an intermediate layer on the colored layer, and a surface layer on the intermediate layer, wherein
- the colored layer contains:
- more than 35 at % to 99 at % or less of C,
- 0 a t% or more to less than 40 at % of Cr,
- 0 at % or more to less than 15 at % of N, and
- more than 0 at % to less than 15 at % of O,
- provided that the total of C, Cr, N, and O is 100 at %,
- in a profile obtained by an XPS depth direction analysis, in a depth region after 8 minutes from when an atomic ratio of Cr, Zr, or Si exceeds that of C;
- and
- the intermediate layer contains at least one metal atom selected from Cr, Zr, and Si;
- and an oxygen atom,
- the metal element in an oxidized state is detected with XPS in the intermediate layer, and
- the intermediate layer exhibits a sputtering time of 0.5 minutes or more to 9 minutes or less, the sputtering time being a time taken from when the metal element is detected to when the amount of the detected oxygen atoms exceeds the amount of the detected oxygen atoms (O) contained in the colored layer, with an XPS depth direction analysis;
- and
- the surface layer
- is water-repellent, and
- includes a hydrophobic group, and
- exhibits, in a profile obtained by the XPS depth direction analysis, a sputtering time of more than 0.5 minutes to 5 minutes or less, the sputtering time being a time taken from when the sputtering starts to when the metal atom contained in the intermediate layer starts to be detected.
Dependencies are inferred from the claim text.