The present invention provides a rare-earth sintered magnet that is characterized in that: R (R indicates one or more elements selected from rare-earth elements, wherein Nd is essential), T (T indicates one or more elements selected from iron-group elements, wherein Fe is essential), X (X indicates one or two elements selected from B and C, wherein B is essential), M1 (M1 indicates one or more elements selected from Al, Si, Cr, Mn, Cu, Zn, Ga, Ge, Mo, Sn, W, Pb, and Bi), 0.1 mass % or less of O, 0.05 mass % or less of N, and 0.07 mass % or less of C are contained; the average crystal grain size is 4.0 μm or less; and relational expression (1) 0.26×D+97≤Or≤0.26×D+99 is satisfied assuming that the degree of orientation is Or [%] and that the average crystal grain size is D [μm]. With this rare-earth sintered magnet, it is possible to achieve superior magnetic characteristics in which both high Br and high HcJ are achieved.
A rare earth sintered magnet comprising R, T, X, and M1 wherein R is at least one element selected from rare earth elements, essentially including Nd, T is at least one element selected from iron group elements, essentially including Fe, X is one or two elements selected from B and C, essentially including B, M1 is at least one element selected from Al, Si, Cr, Mn, Cu, Zn, Ga, Ge, Mo, Sn, W, Pb, and Bi, the magnet containing up to 0.1% by weight of O, up to 0.05% by weight of N, and up to 0.07% by weight of C, and having an average crystal grain size of up to 4.0 μm and a degree of orientation that meets the relationship (1):
Dependencies are inferred from the claim text.