Bearing formed of an aluminum alloy material and method of manufacturing
AssigneeTenneco Inc.
InventorsDavid Michael Saxton, Andrew R. Zeagler, Terri Ann Giroux, Michael Wagner, Katherine Theresa Vaida
Life of this patent
Estimating the term…
Loading patent…
AssigneeTenneco Inc.
InventorsDavid Michael Saxton, Andrew R. Zeagler, Terri Ann Giroux, Michael Wagner, Katherine Theresa Vaida
Estimating the term…
A sliding element, such as a bearing, and a method of manufacturing the sliding element, is provided. The sliding element is formed of an aluminum alloy material which includes zinc in an amount of 5 wt. % to 83 wt. %. The sliding element may also include silicon and/or magnesium. The sliding element is typically formed by casting, heat treating at a temperature of 400° C. to 577° C., and cooling at a rate of less than 50° C. per hour to a temperature ranging from 400° C. to 200° C. The aluminum alloy material is then heat treated at a temperature of 100° to 275° C. for at least 5 hours to form a soft phase consisting essentially of the zinc. The second heat treatment, or possibly both heat treatments, may not be required when the aluminum alloy material includes the magnesium.
A sliding element, comprising:
A method of manufacturing a sliding element, comprising the steps of:
A method of manufacturing a sliding element, comprising the step of:
Dependencies are inferred from the claim text.