Crosslinked pulps, cellulose ether products made therefrom; and related methods of making pulps and cellulose ether products
AssigneeInternational Paper Company
InventorsMengkui Luo, Michael Rea, Angela Dodd, Andrew Dodd, Amy Anderson-Gaber, Kris Lindenauer, Hugh West, Charles Miller
Life of this patent
Estimating the term…
Abstract
Pulps, cellulose ether products, and methods of making pulps are described.
Claims45
A pulp comprising:
- crosslinked cellulose fibers, wherein the pulp has a pulp R18 value greater than or equal to 93%.
A pulp comprising:
- crosslinked cellulose fibers, wherein the pulp has:
- a resultant carboxymethyl cellulose (CMC) viscosity coefficient of variability (COV) of less than 30%;
- and
- a pulp R18 value greater than 92%.
1 more element
A pulp comprising:
- crosslinked cellulose fibers, wherein the pulp has:
- a water retention value (WRV) in a range between 0.8 g/g and less than 1.0 g/g;
- and
- a pulp R18 value greater than 89%.
1 more element
A crosslinked linters pulp having
- an R18 value of 99 or greater, and
- a water retention value in a range between 0.6 g/g and 0.8 g/g.
A method of making a pulp, comprising:
- digesting a cellulosic feedstock to form a pulp;
- bleaching the pulp to form a bleached pulp;
- crosslinking cellulose fibers within the bleached pulp with a crosslinker to form a crosslinked pulp, wherein during crosslinking the bleached pulp has a consistency greater than 30%, and wherein an R18 value of the crosslinked pulp is greater than 92%;
- and
- drying the crosslinked pulp.
2 more elements
A method of making a pulp, comprising:
- contacting wood fibers with a crosslinker and an alkaline hydroxide, wherein the wood fibers have a water content in a range of about 0 wt. % to about 50 wt. %;
- heating the wood fibers, the crosslinker, and the alkaline hydroxide to provide crosslinked wood fibers;
- and
- washing the crosslinked wood fibers to remove unreacted crosslinker and alkaline hydroxide;
- wherein an R18 value of the pulp after crosslinking is greater than or equal to 93%.
2 more elements
A method of making a crosslinked cellulose pulp, comprising:
- activating a cellulosic pulp with an alkali hydroxide at a consistency of greater than 4% to provide an activated pulp;
- removing the alkali hydroxide from the activated pulp;
- and
- crosslinking the activated pulp with a crosslinker at a consistency of greater than 20% and at a temperature in a range of 30° C. to 95° C. to provide a crosslinked pulp.
1 more element