Back to results
US 2022/0294076 A1Published application
Method for Producing Separator for Power Storage Device
AssigneeAsahi Kasei Kabushiki Kaisha
InventorsXun Zhang, Hayato Matsuyama, Tetsushi Nakao
Life of this patent
Estimating the term…
Abstract
Provided is a method for producing a separator for a power storage device, the method including: a step for extruding powdered polyethylene, pelletized polypropylene, and a plasticizer into a sheet form using an extruder to form a molded body; and a step for making the molded body porous by a wet method.
Claims15
A method for producing a separator for a power storage device comprising the following steps:
- (1) a sheet casting step in which polypropylene, polyethylene and a plasticizer are extruded into a sheet using an extruder, cooled to solidification, and processed into a cast sheet;
- (2) a stretching step in which the cast sheet is stretched to an area increase factor of 20 to 250 to form a stretched sheet;
- (3) a microporous membrane forming step in which the plasticizer is extracted from the stretched sheet to form a microporous membrane;
- (4) a heat treatment step in which the microporous membrane is subjected to heat treatment, and stretching and relaxation in the transverse direction to obtain a heat treated microporous membrane;
- and
- (5) a winding step in which the heat treated microporous membrane is wound up,
- wherein the polyethylene is in powder form and the polypropylene is in pellet form.
4 more elements
A separator for a power storage device comprising a microporous membrane, wherein:
- the microporous membrane comprises polyethylene and polypropylene, and
- in X-ray diffraction (XRD) analysis of the microporous membrane, the crystallite size of the polyethylene is 15 nm to 40 nm and the crystallite size of the polypropylene is 10 nm to 50 nm.
A separator for a power storage device comprising a microporous membrane, wherein:
- the microporous membrane comprises polyethylene and polypropylene, and
- in wide-angle X-ray scattering (WAXS) analysis of the microporous membrane, the crystallite size of the polyethylene is 15 nm to 40 nm and the crystallite size of the polypropylene is 10 nm to 50 nm.
Dependencies are inferred from the claim text.