Method for manufacturing secondary battery
AssigneeLG Energy Solution, Ltd.
InventorsYoung Jae KIM, Jung Woo YOO, Ye Lin KIM
Life of this patent
Estimating the term…
Loading patent…
AssigneeLG Energy Solution, Ltd.
InventorsYoung Jae KIM, Jung Woo YOO, Ye Lin KIM
Estimating the term…
A method for manufacturing a secondary battery including: forming an electrode assembly including a negative electrode including a silicon-based active material, a positive electrode facing the negative electrode, and a separator between the negative electrode and the positive electrode; impregnating the electrode assembly by injecting an electrolytic solution into the electrode assembly to form an impregnated electrode assembly; performing activation through first charging/discharging in at least one cycle while pressurizing the impregnated electrode assembly to form an activated electrode assembly; allowing the activated electrode assembly to stand at 40° C. to 80° C. in a state of being charged to a SOC of 70% or more; removing a gas generated from the electrode assembly after allowing the activated electrode assembly to stand; and subjecting the electrode assembly to a second charging/discharging in at least one cycle at 15° C. to 30° C. after the removing of gas generated from the electrode assembly.
A method for manufacturing a secondary battery, the method comprising:
Dependencies are inferred from the claim text.