Electrolyte and Electrode Materials for Rechargeable Lithium Batteries
AssigneeU.S. Army Combat Capabilities Development Command Army Research Laboratory
InventorJan L. Allen
Life of this patent
Estimating the term…
Abstract
A composition of matter and method includes Li1+x+zM(II)0.5−2x−zM(III)x+yM(IV)1.5−2y−zM(V)yM(V)zO4. M(II) includes any of Mg, Co, Ni, Cu, and Zn. M(III) includes any of Al, Cr, Fe, Ga, and In. M(IV) includes any of Ti, Mn, and Ge. M(V) includes any of Nb, Ta, Sb, and Bi. Additionally, 0≤x≤0.25, 0≤y≤0.75, 0≤z≤0.5, and (x+z)>0.
Claims20
A composition of matter comprising Li1+x+zM(II)0.5−2x−zM(III)x+yM(IV)1.5−2y−zM(V)yM(V)zO4, wherein M(II) comprises any of Mg, Co, Ni, Cu, and Zn, wherein M(III) comprises any of Al, Cr, Fe, Ga, and In, wherein M(IV) comprises any of Ti, Mn, and Ge, wherein M(V) comprises any of Nb, Ta, Sb, and Bi, and wherein 0≤x≤0.25, 0≤y≤0.75, 0≤z≤0.5.
A method comprising:
- preparing a compound comprising Li1+x+zM(II)0.5−2x−zM(III)x+yM(IV)1.5−2y−zM(V)yM(V)zO4, wherein M(II) comprises any of Mg, Co, Ni, Cu, and Zn, wherein M(III) comprises any of Al, Cr, Fe, Ga, and In, wherein M(IV) comprises any of Ti, Mn, and Ge, wherein M(V) comprises any of Nb, Ta, Sb, and Bi, and wherein 0≤x≤0.25, 0≤y≤0.75, 0≤z≤0.5;
- dissolution of precursors of the compound into aqueous citric acid and nitric acid to obtain an aqueous solution;
- heating the aqueous solution to form a precipitate;
- and
- heating the precipitate at 400-1100° C.
Dependencies are inferred from the claim text.