Cathode materials, batteries, and methods of forming one or more electrodes for batteries are disclosed. A coated cathode material includes a lithium battery cathode material, a first sub-nanoscale lithium metal oxide coating on the lithium transition metal oxide and a sub-nanoscale metal oxide coating on top of the first sub-nanoscale lithium metal oxide coating. The first sub-nanoscale lithium metal oxide and the sub-nanoscale metal oxide coating are each less than 1 nm thick.
Claims25
A coated cathode material comprising:
- a lithium battery cathode material comprising a lithium transition metal oxide;
- a first sub-nanoscale lithium metal oxide coating on the lithium battery cathode material;
- and
- a second sub-nanoscale metal oxide coating disposed on the first sub-nanoscale lithium metal oxide coating;
- wherein the first sub-nanoscale lithium metal oxide and the second sub-nanoscale metal oxide coating are each less than 1 nm thick.
A method of forming one or more coated cathode materials for a lithium battery, the method comprising:
- providing a lithium battery cathode material;
- coating the lithium battery cathode material with a first sub-nanoscale lithium metal oxide coating;
- and
- coating the lithium battery cathode material with a second sub-nanoscale metal oxide coating on top of the first sub-nanoscale lithium metal oxide coating;
- wherein the first sub-nanoscale lithium metal oxide and the second sub-nanoscale metal oxide coating are each less than 1 nm thick.
A method for an atomic layer deposition on a lithium battery cathode material comprising:
- providing a ball-milling mechanism, the ball-milling mechanism comprising:
- a rotating reactor with a plurality of balls, wherein the plurality of balls comprises one or more of ZrO2, TiO2, stainless steel, and Al2O3;
- performing the atomic layer deposition at a deposition temperature between 20 to 400° C.;
- providing one or more metal precursors, wherein the metal precursors comprise one or more of Al, Ti, Co, Ni, Cu, Si, Ge, Se, Zr, Nb, W, Sn, Ga, Li, Mg, Sr, Ba, Fe, Hf, Ru, Ta, V, Y;
- wherein the atomic layer deposition is performed at a pulse (dose) time for a metal precursor between 0.05 to 60 second to fill the reactor full;
- wherein the atomic layer deposition is performed with one or more pulses (doses) of the same or different metal precursors to form different metal elements on the same layer;
- wherein the atomic layer deposition is performed an exposure time between 1 to 3600 second until saturation;
- wherein the atomic layer deposition is performed for a purge time until it reaches an appropriate vacuum state;
- wherein the atomic layer deposition is performed with H2O and/or ozone to attach oxygen on the metal precursor surface;
- wherein the atomic layer deposition is performed for one or more cycles;
- and
- wherein the metal oxide coating has a thickness of less than 1 nm.