Polyamide 56 fibre with low boiling water shrinkage rate, preparation method therefor, and application thereof
OwnerChaoxu SUN, Xiucai LIUinventors
Life of this patent
Estimating the term…
Loading patent…
OwnerChaoxu SUN, Xiucai LIUinventors
Estimating the term…
The present invention relates to the technical field of polyamide materials, and provides a polyamide 56 pre-oriented yarn and a polyamide 56 draw textured yarn with a low shrinkage in boiling water, a process for producing the same and a use thereof. The raw materials for producing the polyamide 56 fiber comprise 1,5-pentane diamine and adipic acid, or a polyamide 56 resin obtained by polymerizing 1,5-pentane diamine monomer and adipic acid monomer; wherein the polyamide 56 fiber has a shrinkage in boiling water of 9% or less, wherein the polyamide 56 fiber comprises a polyamide 56 pre-oriented yarn with a low shrinkage in boiling water and a polyamide 56 draw textured yarn with a low shrinkage in boiling water. The polyamide 56 fiber has good mechanical properties, dyeing uniformity and dimensional stability. The process for producing the polyamide 56 fiber does not require modification to existing equipments for texturing polyamide fibers and thus reduces production costs.
1-11. (canceled)
A polyamide 56 fiber, characterized in that raw materials for producing the polyamide 56 fiber comprise 1,5-pentane diamine and adipic acid, or a polyamide 56 resin obtained by polymerizing 1,5-pentane diamine monomer and adipic acid monomer;
A process for producing a polyamide 56 pre-oriented yarn, characterized in that the process comprises the following steps:
A process for producing the polyamide 56 draw textured yarn, characterized in that the process comprises the following steps:
Dependencies are inferred from the claim text.