Nickel-containing steel for low temperature
AssigneeNippon Steel Corporation
InventorsTetsuya NAMEGAWA, Manabu HOSHINO, Shinichi OMIYA, Takayuki KAGAYA
Life of this patent
Estimating the term…
Loading patent…
AssigneeNippon Steel Corporation
InventorsTetsuya NAMEGAWA, Manabu HOSHINO, Shinichi OMIYA, Takayuki KAGAYA
Estimating the term…
A Ni steel has a chemical composition within a predetermined range, in which a metallographic structure of a thickness middle portion contains 2.0 vol % to 20.0 vol % of an austenite phase, an average grain size of prior austenite grains is 3.0 μm to 12.0 μm, an average aspect ratio of the prior austenite grains is 2.6 to 10.0, a plate thickness is 4.5 mm to 20 mm, a yield stress at room temperature is 590 MPa to 710 MPa, and a tensile strength at the room temperature is 690 MPa to 810 MPa, when the plate thickness is more than 16 mm, the Ni steel contains Ni: 11.5% or more, and when the plate thickness is 16 mm or less and the Ni steel contains Ni: less than 11.5%, the average grain size of the prior austenite grains is 6.0 μm or less.
A nickel-containing steel comprising, as a chemical composition, by mass %:
Dependencies are inferred from the claim text.