Back to results
US 2022/0282352 A1Published application
Thin steel plate having excellent low-temperature toughness and ctod properties, and method for manufacturing same
AssigneePosco
InventorsWoo-Gyeom Kim, Sang-Ho Kim, Ki-Hyun Bang
Life of this patent
Estimating the term…
Abstract
The present invention relates to structural steel that can be desirably used in offshore structures and the like, more specifically, to a thin steel plate having excellent low-temperature toughness and CTOD properties, and to a method for manufacturing the same.
Claims9
A thin steel plate having excellent low-temperature toughness and CTOD properties, the thin steel plate comprising, by weight:
- 0.05 to 0.1% of carbon (C), 0.05 to 0.3% of silicon (Si), 1.0 to 2.0% of manganese (Mn), 0.005 to 0.04% of aluminum (Sol. Al), 0.005 to 0.03% of niobium (Nb), 0.005 to 0.02% of titanium (Ti), 0.05 to 0.4% of copper (Cu), 0.3 to 1.0% of nickel (Ni), 0.001 to 0.008% of nitrogen (N), 0.01% or less of phosphorus (P), and 0.003% or less of sulfur (S), with a balance of Fe and other unavoidable impurities,
- wherein the thin steel plate includes acicular ferrite (water-cooled ferrite) having an area fraction of 30 to 50% and polygonal ferrite (air-cooled ferrite) having an area fraction of 50 to 70% as a microstructure, and
- has a thickness of 8 to 30 mm.
A manufacturing method of a thin steel plate having excellent low-temperature toughness and CTOD properties, the method comprising:
- heating a steel slab including, by weight:
- 0.05 to 0.1% of carbon (C), 0.05 to 0.3% of silicon (Si), 1.0 to 2.0% of manganese (Mn), 0.005 to 0.04% of aluminum (Sol. Al), 0.005 to 0.03% of niobium (Nb), 0.005 to 0.02% of titanium (Ti), 0.05 to 0.4% of copper (Cu), 0.3 to 1.0% of nickel (Ni), 0.001 to 0.008% of nitrogen (N), 0.01% or less of phosphorus (P), and 0.003% or less of sulfur (S), with a balance of Fe and other unavoidable impurities to 1200° C. or higher;
- rough rolling the heated steel slab at 1000° C. or higher;
- after the rough rolling, finish-hot-rolling the steel slab at a temperature equivalent to or higher than Ar3 to manufacture a hot-rolled steel plate;
- air-cooling the hot-rolled steel plate;
- and
- after the air cooling, cooling the hot-rolled steel plate at a cooling rate of 10 to 30° C./s,
- wherein the cooling is water cooling, and starts in a temperature range of 660 to 690° C. and ends in a temperature range of 550 to 590° C., and the thin steel plate has a thickness of 8 to 30 mm.
5 more elements
Dependencies are inferred from the claim text.