Method for manufacturing a high strength steel product and steel product thereby obtained
AssigneeArcelorMittal
InventorsArtem Arlazarov, Kangying Zhu
Life of this patent
Estimating the term…
Loading patent…
AssigneeArcelorMittal
InventorsArtem Arlazarov, Kangying Zhu
Estimating the term…
A method for manufacturing a steel product, comprising the steps of: providing a heated steel starting product at a temperature comprised between 380° C. and 700° C., having a metastable fully austenitic structure, with a composition comprising, in percent by weight: 0.15%≤C≤0.40%, 1.5%≤Mn≤4.0%, 0.5%≤Si≤2.5%, 0.005%≤Al≤1.5%, with 0.8%≤Si+Al≤2.5%, S≤0.05%, P≤0.1%, at least one element chosen among Cr and Mo, such that: 0%≤Cr≤4.0%, 0%≤Mo≤0.5%, and 2.7%≤Mn+Cr+3 Mo≤5.7%, and optionally one or several elements chosen among: Nb≤0.1%, Ti≤0.1%, Ni≤3.0%, 0.0005%≤B≤0.005%, 0.0005%≤Ca≤0.005%, the balance of the composition consisting of iron and unavoidable impurities resulting from the smelting; subjecting said starting product to a hot forming step at a temperature comprised between 700° C. and 380° C., with a cumulated strain εb between 0.1 and 0.7, in at least one location of said heated steel starting product, to obtain a fully austenitic hot-formed steel product; then quenching the hot-formed steel product by cooling it down, at a cooling rate VR2 superior to the critical martensitic cooling rate, to a quenching temperature QT lower than Ms in order to obtain a structure containing between 40% and 90% of martensite, the rest of the structure being austenite; then maintaining at, or reheating the product up to a holding temperature PT between QT and 470° C. and holding it at said temperature PT for a duration Pt between 5 s and 600 s.
A steel product having a composition comprising, in percent by weight:
Dependencies are inferred from the claim text.