Method for producing thermoplastically processable polyurethane polymers
AssigneeCovestro Intellectual Property GmbH & Co. KG
InventorsYi Shen, Franz-Heinrich Hermanns, Christian Wamprecht, Peter Reichert
Life of this patent
Estimating the term…
Abstract
The present invention relates to a novel process for preparing thermoplastically processable polyurethanes, to thermoplastically processable polyurethane obtainable from the process and to compositions, articles and uses of these polyurethanes.
Claims20
A solvent-free process for preparing thermoplastically processable polyurethane polymers by reacting the following components
- (A) one or more essentially linear polyols, wherein a total amount of component (A) has an average molecular weight Mn in a range from 500 g/mol to 5000 g/mol, wherein Mn is calculated from the OH number determined according to DIN53240;
- (B) one or more organic polyisocyanates;
- (C) one or more linear diols having a molecular weight of 62 g/mol to 500 g/mol;
- (D) optionally in the presence of one or more catalysts;
- (E) optionally in the presence of additives, auxiliaries, additions, or a combination thereof;
- and
- (F) optionally in the presence of one or more monofunctional chain terminators,
- wherein the process comprises:
- 1) providing and reacting a mixture comprising the total amount of component (A), a subamount of component (B), and optionally a subamount or a total amount of component (D), component (E), component (F), or a combination thereof to afford an NCO-functional prepolymer, wherein in process step 1) a molar ratio of component (B) to component (A) is in a range from 1.1:1.0 to 5.0:1.0;
- 2) reacting the NCO-functional prepolymer from process step 1) with a total amount of component (C) to obtain an OH-functional prepolymer, optionally in the presence of a further subamount of component (D), component (E), component (F), or a combination thereof;
- and
- 3) reacting the OH-functional prepolymer from process step 2) with a remaining amount of component (B) and any remaining amount of component (D), component (E), component (F), or a combination thereof to obtain the thermoplastically processable polyurethane, wherein over all process steps a molar ratio of component (B) to a sum of component (A) and component (C) is in a range from 0.9:1.0 to 1.2:1.0.
A thermoplastically processable polyurethane polymer having a Charpy impact strength of ≥15 KJ/m2 at −30° C. determined according to DIN EN ISO179/1eA, obtained by reacting the following components
- (A) one or more essentially linear polyether diols based on a polymer of tetrahydrofuran, wherein a total amount of component (A) has an average molecular weight Mn of greater than 1450 g/mol, wherein Mn is calculated from the OH number determined according to DIN53240;
- (B) one or more organic polyisocyanates;
- (C) one or more linear diols having a molecular weight of 62 g/mol to 500 g/mol;
- (D) optionally in the presence of one or more catalysts;
- (E) optionally in the presence of one or more additives, auxiliaries, additions, or a combination thereof;
- and
- (F) optionally in the presence of one or more monofunctional chain terminators,
- wherein the reaction of the components is performed in a solvent-free fashion and comprises the following steps:
- 1. providing and reacting a mixture comprising the total amount of component (A), a subamount of component (B), and optionally a subamount or a total amount of component (D), component (E), component (F), or a combination thereof to afford an NCO-functional prepolymer, wherein in process step 1) a molar ratio of component (B) to component (A) is in the range from 1.1:1.0 to 5.0:1.0;
- 2. reacting the NCO-functional prepolymer from process step 1) with a total amount of component (C) to obtain an OH-functional prepolymer, optionally in the presence of a further subamount of component (D), component (E), component (F), or a combination thereof;
- and
- 3. reacting the OH-functional prepolymer from process step 2) with a remaining amount of component (B) and any remaining amount of component (D), component (E), component (F), or a combination thereof to obtain the thermoplastically processable polyurethane, wherein over all process steps a molar ratio of component (B) to a sum of component (A) and component (C) is in a range from 0.9:1.0 to 1.2:1.0.
Dependencies are inferred from the claim text.