Chemically strengthened glass and manufacturing method thereof
AssigneeAGC Inc.
InventorsKaname SEKIYA, Yusuke FUJIWARA
Life of this patent
Estimating the term…
Abstract
The present invention relates to a chemically strengthened glass having a thickness t (mm), in which a first-order derivative CSx′ of a stress value CSx (MPa) is −4.7 or larger in a range of CSx≥0 in a profile of the stress value CSx (MPa), in which the stress value CSx (MPa) is a function of depth×(μm) from a glass surface, and in which the stress value CSx (MPa) is measured by a scattered light photoelastic stress meter, and a manufacturing method thereof.
Claims32
A chemically strengthened glass having a thickness t (mm), wherein a first-order derivative CSx′ of a stress value CSx (MPa) is −4.7 or larger in a range of CSx≥0 in a profile of the stress value CSx (MPa),
- wherein the stress value CSx (MPa) is a function of depth×(μm) from a glass surface, and
- wherein the stress value CSx (MPa) is measured by a scattered light photoelastic stress meter.
A manufacturing method for a chemically strengthened glass, the method comprising:
- performing a first ion exchange by immersing a lithium-containing glass in a first molten salt composition containing sodium ions;
- and
- performing a second ion exchange by immersing the lithium-containing glass obtained after the first ion exchange in a second molten salt composition containing potassium ions and lithium ions, wherein:
- a concentration of a sodium nitrate in the first molten salt composition is higher than 50 mass %;
- and
- in the second molten salt composition a concentration of a potassium nitrate is 85 mass % or higher and a ratio of a mass of sodium ions to a mass of lithium ions represented by a mass ratio of (sodium ions)/(lithium ions) is 0 or larger and 15 or smaller.
A manufacturing method for a chemically strengthened glass, the method comprising:
- performing a first ion exchange by immersing a lithium-containing glass in a first molten salt composition containing sodium ions;
- and
- performing a second ion exchange by immersing the lithium-containing glass obtained after the first ion exchange in a second molten salt composition containing potassium ions and lithium ions, wherein:
- the lithium-containing glass is chemically strengthened so that a maximum tensile stress CT2 (MPa) of the chemically strengthened glass obtained after the second ion exchange becomes 50% to 99% of a maximum tensile stress CT1 (MPa) of the chemically strengthened glass obtained after the first ion exchange.
A manufacturing method for a chemically strengthened glass, the method comprising:
- a first step of immersing a lithium-containing glass in a first molten salt composition;
- and
- a second step of immersing the lithium-containing glass in a second molten salt composition that is different in composition from the first molten salt composition, wherein:
- an ion exchange for giving a stress that is larger than a CT limit to the lithium-containing glass is performed in the first step;
- and
- a step of reducing the stress to a value lower than the CT limit is executed in the second step.
A chemically strengthened glass, wherein:
- a base composition comprises, as represented by mol % based on oxides,
- SiO2 of 40% to 75%;
- Al2O3 of 1% to 20%;
- and
- Li2O of 5% to 35%;
- and
- wherein a stress value CS90 at a depth 90 (μm) from a glass surface satisfies the following inequality:
- CS90/{CT2×(t−2×DOL/1,000)}/t≥2.00
- where t (mm) is a thickness of the chemically strengthened glass, CT2 (MPa) is maximum tensile stress and DOL (μm) is a compressive stress layer depth.
Dependencies are inferred from the claim text.