The specification relates to a clay having kaolinite from 20-40 wt. %; illite from 15-30 wt. %; pigeonite from 5-15 wt. %; and quartz up to a maximum of 40 wt. %. The clay is for use as an agent for reducing concentration of phosphorous in a fluid. Also disclosed is a process for preparation of a modified clay, and a method of treatment of a fluid using the clay or modified clay.
Claims16
A clay, the clay comprising:
- kaolinite from 20-40 wt. %;
- illite from 15-30 wt. %;
- pigeonite from 5-15 wt. %;
- and
- quartz up to a maximum of 40 wt. %,
- wherein the clay is for use as an agent for reducing concentration of phosphorous in a fluid.
3 more elements
A method of treatment for reducing the concentration of phosphorous in a fluid, the method comprising:
- contacting the fluid with a clay, or modified clay, comprising:
- kaolinite from 20-40 wt. %;
- illite from 15-30 wt. %;
- pigeonite from 5-15 wt. %;
- and
- quartz up to a maximum of 40 wt. %.
3 more elements
A method of manufacture of a modified clay, the modified clay having kaolinite from 20-40 wt. %;
- illite from 15-30 wt. %;
- pigeonite from 5-15 wt. %;
- and quartz up to a maximum of 40 wt. %, the method comprising:
- calcinating clay at a temperature of from 400 to 700° C. to form the modified clay.