Secondary battery electrode and method for producing the electrode
AssigneePrime Planet Energy & Solutions, Inc.
InventorsNaohiro MASHIMO, Katsushi ENOKIHARA, Haruka SHIONOYA
Life of this patent
Estimating the term…
Abstract
According to the present disclosure, an electrode having both high energy density and ion diffusivity is provided. The electrode disclosed herein includes an electrode active material layer on either a positive- or negative-electrode current collector, in which the electrode active material layer has a concave/convex shape on its surface in a predetermined pattern at a constant pitch. In a cross-sectional SEM image of the electrode active material layer, linear cracks are unevenly distributed in a concave portion compared to in a convex portion.
Claims7
A secondary battery electrode that is either a positive or negative electrode of a secondary battery, the secondary battery electrode comprising:
- an electrode current collector;
- and
- an electrode active material layer formed on the electrode current collector, wherein
- the electrode active material layer has a concave/convex shape on its surface in a predetermined pattern at a constant pitch, and
- in a cross-sectional SEM image of the electrode active material layer, linear cracks are unevenly distributed in a concave portion compared to in a convex portion.
A method for producing an electrode including either a positive- or negative-electrode current collector and either a positive- or negative-electrode active material layer, the method including the following steps:
- a step in which a moisture powder formed by aggregated particles containing at least an electrode active material, a binder resin, and a solvent is prepared,
- here, in the moisture powder, at least 50% by number or more of the aggregated particles form a pendular state or a funicular state in a solid phase, a liquid phase, and a gas phase;
- a step in which a coating film composed of the moisture powder is formed using the moisture powder on the electrode current collector while leaving a gas phase of the coating film;
- a step in which a concave/convex shape is formed with a predetermined pattern and a constant pitch on a surface part of the coating film with the gas phase;
- a step in which the coating film which the concave/convex shape is dried, to form an electrode active material layer;
- and
- a step in which the electrode active material layer is pressed;
- wherein
- here, in the pressing step, pressing is performed such that the linear cracks observed in a cross-sectional SEM image of the electrode active material layer are unevenly distributed in a concave portion compared to in a convex portion.
Dependencies are inferred from the claim text.