Cellulose fibril-enhanced repair mortars
AssigneePerformance Biofilaments Inc.
InventorsGurminder MINHAS, Keith GOURLAY, Nemkumar BANTHIA, Obinna ONUAGULUCHI
Life of this patent
Estimating the term…
Loading patent…
AssigneePerformance Biofilaments Inc.
InventorsGurminder MINHAS, Keith GOURLAY, Nemkumar BANTHIA, Obinna ONUAGULUCHI
Estimating the term…
Repair mortar and methods of preparing repair mortar are provided. The repair mortar comprise a cement binder, fine aggregate and cellulose fibrils. In some embodiments, the cellulose fibrils are dispersed uniformly throughout the repair mortar. In some embodiments, the cellulose fibrils comprise nanofibrillated cellulose and/or microfibrillated cellulose. In some embodiments, the cellulose fibrils comprise an aspect ratio of between about 20 to about 500. The methods comprise mixing a cement binder, fine aggregate with water/chemical admixture to provide a cementitious material of good consistency, mixing cellulose fibrils with water to provide a cellulose fibril slurry, and mixing the cellulose fibril slurry with the workable cementitious material. In some embodiments, the cellulose fibrils are dispersed uniformly throughout the workable cementitious material.
1-41. (canceled)
A repair mortar comprising a cement binder, fine aggregate and cellulose fibrils, wherein the cellulose fibrils are dispersed uniformly throughout the repair mortar, wherein the cellulose fibrils comprise nanofibrillated cellulose and/or microfibrillated cellulose, wherein the cellulose fibrils comprise an aspect ratio of between about 20 to about 500, wherein the cellulose fibrils have a width of between about 20 nm to about 30 μm, wherein the cellulose fibrils have a length of between about 1 μm to about 2,000 μm, wherein the cellulose fibrils comprise between about 0.05 vol. % and about 5 vol. %, or about 0.1 vol % of the repair mortar, and wherein the surface area of the cellulose fibrils is between 60-100 m2/g.
The repair mortar according to claim 1 wherein the cement binder comprises between about 20 vol. % to about 22 vol. % of the repair mortar, and a water to cement binder ratio of between about 0.2 to about 0.6, wherein the cement binder comprises one or more of a filler, a chemical admixture, and a moisture-retaining agent, and wherein the filler comprises one or more of sand, calcium carbonate, limestone, crushed stone, and gravel, and wherein the filler comprises between about 45 vol. % and about 55 vol. % of the repair mortar, wherein the chemical admixture comprises one or more of an air-entraining agent, retarding agent, accelerating agent, plasticizer, polymer, corrosion inhibitor, alkali-silica reactivity reduction agent, bonding agent, coloring agent, defoamer, odor-masking agent, and dry dispersing agent, wherein the chemical admixture comprises between about 0.03 vol. % and about 0.3 vol. % of the repair mortar, wherein the moisture-retaining agent comprises a co-polymer comprising one or more of hydroxypropyl methylcellulose (HPMC), hydroxyethyl methylcellulose (HEMC), welan and xanthan gums, and wherein the moisture-retaining agent comprises between about 0 vol. % and about 0.08 vol. % of the repair mortar.
A method of preparing a repair mortar, the method comprising:
A method of improving corrosion resistance of rebar in concrete material being repaired with repair mortar, the method comprising:
Dependencies are inferred from the claim text.