Back to results
US 2022/0045361 A1Published application
Solid electrolyte for organic batteries
AssigneeEvonik Operations GmbH
InventorsAndreas Wild, Michael Korell, Simon Münch, Alexandra Lex-Balducci, Johannes Brendel, Ulrich Sigmar Schubert
Life of this patent
Estimating the term…
Abstract
A process can be used to produce a charge storage unit, especially a secondary battery, the electrodes of which contain an organic redox-active polymer, and which includes a polymeric solid electrolyte. The solid electrolyte is obtained by polymerizing from mixtures of acrylates with methacrylates in the presence of at least one ionic liquid, which imparts advantageous properties to the charge storage unit.
Claims22
1:
- A process for producing a charge storage unit, the process comprising:
- (a) polymerizing a mixture M comprising at least one compound of the formula (I), at least one compound of the formula (II):
- wherein RA, RM are independently selected from the group consisting of hydrogen, an alkyl group, a (poly)ether group, W aryl group, an aralkyl group, an alkaryl group, and a haloalkyl group,
- and at least one ionic liquid IL, to obtain a polymer electrolyte Pele, and
- (b) disposing the polymer electrolyte Pele obtained in (a) between two electrodes Ecat and Ean, wherein Ecat and Ean each independently comprise at least one conductivity additive L and at least one organic redox-active polymer Predox.
2 more elements
2:
- The process according to claim 1, wherein, in (a), a molar ratio of all compounds of formula (I) included in the mixture M to all compounds of the formula (II) included in the mixture M is in the range of 99:1 to 1:99.
3:
- The process according to claim 1, wherein the ionic liquid IL has a structure Q+A− in which Q+ is a cation selected from the group consisting of the structures (Q1), (Q2), (Q3), (Q4), and (Q5)
- wherein RQ1, RQ2, RQ3, RQ4, RQ5, RQ6, RQ7, RQ8 are each independently selected from the group consisting of an alkyl group, a haloalkyl group, and a cycloalkyl group,
- wherein RQ9, RQ10, RQ11, RQ12, RQ13, RQ14, RQ15, RQ16, RQ17, RQ18, RQ19, RQ20, RQ21, RQ22, RQ23, RQ24, RQ25, RQ26, RQ27, RQ28, RQ29, RQ30, RQ31, RQ32, RQ33, RQ34, RQ35 are each independently selected from the group consisting of hydrogen, an alkyl group, a (poly)ether group, a haloalkyl group, and a cycloalkyl group, and
- in which A− is an anion.
1 more element
4:
- The process according to claim 1, wherein a total molar amount of all ionic liquids IL included in the mixture M in (a), based on a total molar amount of all compounds of the formulae (I) and (II) included in the mixture M, is ≥0.1 molar equivalent.
5:
- The process according to claim 1, wherein (a) is conducted on a surface of at least one of the electrodes Ecat and Ean.
6:
- The process according to claim 1, wherein the polymer Predox is selected from the group consisting of polyimides and polymers comprising m units of the general formula (III):
- wherein m is an integer ≥4, W is a repeat unit, Sp is an organic spacer and RX is an organic redox-active group, wherein the bond identified by (i) in a unit of the formula (III) binds to the bond identified by (ii) in an adjacent unit of the formula (III).
7:
- The process according to claim 6, wherein the polymer Predox is a polymer comprising m units of the general formula (III) in which RX is selected from the group consisting of compounds of the general formulae (III-A), (III-B), (II-C), a (III-D), where
- and wherein, in the structures (III-A), (III-B) and (III-C), at least one aromatic carbon atom may be substituted by a group selected from the group consisting of an alkyl group, a halogen group, an alkoxy group, and a hydroxyl group.
8:
- The process according to claim 6, wherein the polymer Predox is a polyimide selected from the group consisting of the structures (IV-1), (IV-2), (IV-3), (IV4), (IV-5), (IV-6), and (IV-7):
- wherein n in each case is an integer ≥4 and the bond identified by (iv) in the structures (IV-1), (IV-2), (IV-3), (IV4), (IV-5), (IV-6), (IV-7) binds in each case to the bond identified by (v), and
- wherein, in the structures (IV-1), (IV-2), (IV-3), (IV-4), (IV-5), (IV-6), (IV-7), at least one aromatic carbon atom may be substituted by a group selected from the group consisting of alkyl, halogen, alkoxy, and OH.
9:
- The process according to claim 6, wherein the W radical in the structure (III) is selected from the group consisting of the structures (W1), (W2), and (W3):
- wherein the bond identified by (i) in a unit of the formula (W1), (W2), or (W3) binds in each case to the bond identified by (ii) in an adjacent unit of the formula (W1), (W2) or (W3),
- wherein the bond identified by (iii) in each case indicates the bond to Sp, and
- wherein RW1, RW2, RW3, RW4, RW5, RW6, RW7 are independently selected from the group consisting of hydrogen, an alkyl group, a haloalkyl group, and —COORW8 wherein RW8=H or alkyl, and
- wherein Sp in the structure (III) is selected from the group consisting of a direct bond, (Sp1), and (Sp2):
- -(O)pA1—[C═O]pA2—(O)pA3—BSp—(O)qA1—[C═O]qA2—(O)qA3, (Sp1):
- -(O)qA4[C═O]qA5—(O)qA6 (Sp2):
- wherein pA1, pA2, pA3 in each case is 0 or 1, excluding the case that pA2=0 and pA1=pA3=1,
- wherein qA1, qA2, qA3 in each case is 0 or 1, excluding the case that qA2=0 and qA1=qA3=1,
- wherein qA4, qA5, qA6 in each case is 0 or 1, where at least one of qA4, qA5, qA6=1 and excluding the case that qA5=0 and qA4=qA6=1,
- wherein BSp is selected from the group consisting of
- a divalent (hetero)aromatic radical, and
- a divalent aliphatic radical, optionally substituted by at least one group selected from the group consisting of a nitro group, —NH2, —CN, —SH, —OH, and halogen;
- and optionally having at least one group selected from the group consisting of an ether, a thioether, n amino ether, a carbonyl group, a carboxylic ester, a carboxamide group, a sulfonic ester, and a phosphoric ester, and
- where in the cases in which Sp binds to a non-carbon atom in the RX radical, the structure (Sp1) is subject to the additional condition qA3=0, qA2=1, and qA1=1;
- or qA3=qA2=qA1=0;
- or qA3=0, qA2=1, and qA1=0, and the structure (Sp2) is subject to the additional condition that qA6=0, qA5=1, and qA4=1;
- or qA6=0, qA5=1, and qA4=0, and
- wherein denotes the bond pointing toward RX, and
- wherein denotes the bond pointing toward W.
17 more elements
10:
- The process according to claim 1, wherein the polymer Predox comprises t repeat units joined to one another, selected from the group consisting of the structures P1, P2, and P3:
- wherein t is an integer ≥4, and
- the bond identified by (vi) in a unit of the formula P1 binds to the bond identified by (vii) in an adjacent unit of the formula P1, and
- the bond identified by (viii) in a unit of the formula P2 binds to the bond identified by (ix) in an adjacent unit of the formula P2, and
- the bond identified by (x) in a unit of the formula P3 binds to the bond identified by (xi) in an adjacent unit of the formula P3.
2 more elements
11:
- The process according to claim 1, wherein the conductivity additive L is selected from the group consisting of carbon materials, electrically conductive polymers, metals, semimetals, metal compounds, and semimetal compounds.
12:
- A charge storage unit obtainable by the process according to claim 1.
13:
- A charge storage unit, comprising a polymer electrolyte Pele disposed between two electrodes Ecat and Ean, wherein Ecat and Ean each independently comprise at least one conductivity additive L and at least one organic redox-active polymer Predox,
- wherein
- the polymer electrolyte Pele is obtained by polymerizing a mixture M comprising at least one compound of the formula (I), at least one compound of the formula (II):
- wherein RA, RM are independently selected from the group consisting of hydrogen, an alkyl group, a (poly)ether group, an aryl group, an aralkyl group, an alkaryl group, and a haloalkyl group,
- and at least one ionic liquid IL.
2 more elements
14:
- The charge storage unit according to claim 13, wherein a molar ratio of all compounds of formula (I) included in the mixture M to all compounds of the formula (II) included in the mixture M is in the range of 99:1 to 1:99.
15:
- The charge storage unit according to claim 13, wherein the ionic liquid IL has a structure Q+A− in which Q+ is a cation selected from the group consisting of the structures (Q1), (Q2), (Q3), (Q4), and (Q5):
- wherein RQ1, RQ2, RQ3, RQ4, RQ5, RQ6, RQ7, RQ8 are each independently selected from the group consisting of an alkyl group, a haloalkyl group, and a cycloalkyl group,
- wherein RQ9, RQ10, RQ11, RQ12, RQ13, RQ14, RQ15, RQ16, RQ17, RQ18, RQ19, RQ20, RQ21, RQ22, RQ23, RQ24, RQ25, RQ26, RQ27, RQ28, RQ29, RQ30, RQ31, RQ32, RQ33, RQ34, RQ35 are each independently selected from the group consisting of hydrogen, an alkyl group, a (poly)ether group, a haloalkyl group, and a cycloalkyl group, and
- in which A− is an anion.
1 more element
16:
- The charge storage unit according to claim 13, wherein a total molar amount of all ionic liquids IL included in the mixture M, based on g total molar amount of all compounds of the formulae (I) and (II) included in the mixture M, is ≥0.1 molar equivalents.
17:
- The charge storage unit according to claim 13, wherein the polymer Predox is selected from the group consisting of polyimides and polymers comprising m units of the general formula (III):
- wherein m is an integer ≥4, W is a repeat unit, Sp is an organic spacer and RX is an organic redox-active group, wherein the bond identified by (i) in a unit of the formula (III) binds to the bond identified by (ii) in an adjacent unit of the formula (III).
18:
- The charge storage unit according to claim 17, wherein the polymer Predox is a polymer comprising m units of the general formula (III) in which RX is selected from the group consisting of compounds of the general formulae (III-A), (III-B), (III-C), and (III-D), where
- and wherein, in the structures (III-A), (III-B) and (III-C), at least one aromatic carbon atom may be substituted by a group selected from the group consisting of alkyl, halogen, alkoxy, d OH.
19:
- The charge storage unit according to claim 17, wherein the polymer Predox is a polyimide selected from the group consisting of the structures (IV-1), (IV-2), (IV-3), (IV-4), (IV-5), (IV-6), ad (IV-7):
- wherein, n in each case is an integer ≥4 and the bond identified by (iii) in the structures (IV-1), (IV-2), (IV-3), (IV-4), (IV-5), (IV-6), (IV-7) binds in each case to the bond identified by (iv), and
- wherein, in the structures (IV-1), (IV-2), (IV-3), (IV-4), (IV-5), (IV-6), (IV-7), at least one aromatic carbon atom may be substituted by a group selected from the group consisting of alkyl, halogen, alkoxy, and OH.
20:
- The charge storage unit according to claim 17, wherein the W radical in the structure (III) is selected from the group consisting of the structures (W1), (W2), an (W3):
- wherein the bond identified by (i) in a unit of the formula (W1), (W2), gr (W3) binds in each case to the bond identified by (ii) in adjacent unit of the formula (W1), (W2) or (W3),
- wherein the bond identified by (iii) in each case indicates the bond to Sp, and
- wherein RW1, RW2, RW3, RW4, RW5, RW6, RW7 are independently selected from the group consisting of hydrogen, a alkyl group, g haloalkyl group, and —COORW8 wherein RW8=H or alkyl, and
- wherein Sp in the structure (III) is selected from the group consisting of a direct bond, (Sp1), n (Sp2):
- -(O)pA1—[C═O]pA2—(O)pA3—BSp—(O)qA1—[C═O]qA2—(O)qA3, (Sp1):
- -(O)qA4—[C═O]qA5—(O)qA6- (Sp2):
- wherein pA1, pA2, pA3 in each case is 0 or 1, excluding the case that pA2=0 and pA1=pA3=1,
- wherein qA1, qA2, qA3 in each case is 0 or 1, excluding the case that qA2=0 and qA1=qA3=1,
- wherein qA4, qA5, qA6 in each case is 0 or 1, where at least one of qA4, qA5, qA6=1 and excluding the case that qA5=0 and qA4=qA6=1,
- wherein BSp is selected from the group consisting of
- a divalent (hetero)aromatic radical, and
- a divalent aliphatic radical, optionally substituted by at least one group selected from the group consisting of a nitro group, —NH2, —CN, —SH, —OH, nd halogen;
- and optionally having at least one group selected from the group consisting of an ether, a thioether, n amino ether, a carbonyl group, a carboxylic ester, a carboxamide group, a sulfonic ester, and a phosphoric ester, and
- where in the cases in which Sp binds to a non-carbon atom in the RX radical, the structure (Sp1) is subject to the additional condition qA3=0, qA2=1, And qA1=1;
- or qA3=qA2=qA1=0;
- or qA3=0, qA2=1, M qA1=0, and the structure (Sp2) is subject to the additional condition that qA6=0, qA5=1, and qA4=1;
- or qA6=0, qA5=1, and qA4=0, and
- wherein denotes the bond pointing toward RX, and
- wherein denotes the bond pointing toward W.
17 more elements
21:
- The charge storage unit according to claim 13, wherein the polymer Predox comprises t repeat units joined to one another, selected from the group consisting of the structures P1, P2, and P3:
- wherein t is an integer ≥4, and
- the bond identified by (vi) in a unit of the formula P1 binds to the bond identified by (vii) in an adjacent unit of the formula P1, and
- the bond identified by (viii) in a unit of the formula P2 binds to the bond identified by (ix) in an adjacent unit of the formula P2, and
- the bond identified by (x) in a unit of the formula P3 binds to the bond identified by (xi) in an adjacent unit of the formula P3.
2 more elements
22: