Drawn composite fiber, non-woven fabric, and method of producing drawn composite fiber
AssigneeUbe Exsymo Co., Ltd.
InventorsSatoshi KUSAKA, Kotaro TOMITA
Life of this patent
Estimating the term…
Loading patent…
AssigneeUbe Exsymo Co., Ltd.
InventorsSatoshi KUSAKA, Kotaro TOMITA
Estimating the term…
Embodiments relate to a drawn composite fiber having a low thermal shrinkage, and a high single yarn strength, a non-woven fabric using the same, and a method of producing the same. The drawn composite fiber has a fineness of 0.6 dtex or less, a ratio between the cross-sectional areas of a sheath material and a core material (sheath material/core material) of 50/50 to 10/90, and a single yarn elastic modulus of 70 cN/dtex or more. The drawn composite is obtained by melt-spinning and a drawing treatment of an undrawn fiber having a sheath-core structure, in which the core material includes a resin containing a crystalline propylene-based polymer and having a melt flow rate of 10 to 30 g/10 min at a load of 21.18 N at 230° C., and the sheath material includes a resin containing an olefinic polymer where the melting point is lower than that of the core material.
A drawn composite fiber comprising a sheath-core structure in which a resin containing a crystalline propylene-based polymer as a main component is a core material, and a resin containing, as a main component, an olefinic polymer of which a melting point is lower than that of the core material is a sheath material, wherein
A method of producing a drawn composite fiber, comprising:
Dependencies are inferred from the claim text.