Hot-forged tial-based alloy, method for producing same, and uses for same
AssigneeNational Institute for Materials Science
InventorToshimitsu TETSUI
Life of this patent
Estimating the term…
Abstract
The present invention provides a TiAl-based alloy, including: Al: 41 to 43 at %; Fe: 0 to 2.5 at %; Ni: 0 to 2.5 at %; Mo: 0 to 2.0 at %; W: 0 to 2.0 at %; Cr: 0 to 4.5 at %; Mn: 0 to 5.5 at %; V: 0 to 10 at %; Nb: 0 to 10 at %; C: 0.3 to 0.7 at %; and a remainder consisting of Ti and inevitable impurities, in which an alloy element parameter “P=(41.5−Al)/3+Fe+Ni+Mo+W+0.5 Cr+0.4 Mn+0.2 V+0.2 Nb—C” is in a composition range of 1.1 to 1.9, and the TiAl-based alloy has a microstructure consisting of a γ phase of 5 to 30 area %, a β phase of 0.5 to 5 area %, and a lamellar structure occupying a remaining part.
Claims7
A TiAl-based alloy, comprising:
- Al:
- 41 to 43 at %;
- Fe:
- 0 to 2.5 at %;
- Ni:
- 0 to 2.5 at %;
- Mo:
- 0 to 2.0 at %;
- W:
- 0 to 2.0 at %;
- Cr:
- 0 to 4.5 at %;
- Mn:
- 0 to 5.5 at %;
- V:
- 0 to 10 at %;
- Nb:
- 0 to 10 at %;
- C:
- 0.3 to 0.7 at %;
- and
- a remainder consisting of Ti and inevitable impurities,
- wherein an alloy element parameter P obtained by Equation (1) below is in a composition range of 1.1 to 1.9, and
- the TiAl-based alloy has a microstructure consisting of a γ phase of 5 to 30 area %, a β phase of 0.5 to 5 area %, and a lamellar structure occupying a remaining part,
- P=(41.5−Al)/3+Fe+Ni+Mo+W+0.5 Cr+0.4 Mn+0.2 V+0.2 Nb—C (1).
Dependencies are inferred from the claim text.