US 2022/0010419 A1Published application
Multi-process hardening method
OwnerMatthew W. Simoneinventor
Life of this patent
Estimating the term…
Abstract
Embodiments of multi-process hardened golf club heads and methods of multi-process hardening of golf club heads are generally described herein. Other embodiments and methods may be described and claimed.
Claims20
A method of a club head assembly, the method comprising:
- (a) providing a golf club head having a recess, and providing a faceplate, wherein the golf club head and the faceplate are formed from an α-β Ti alloy, the α-β Ti alloy comprising between 5.5 wt % to 6.75 wt % aluminum (Al), between 3.5 wt % to 4.5 wt % vanadium (V), a maximum of 0.08 wt % carbon (C), a maximum of 0.03 wt % silicon (Si), a maximum of 0.3 wt % iron (Fe), a maximum of 0.2 wt % oxygen (O), a maximum of 0.015 wt % tin (Sn), and a trace of molybdenum (Mo);
- (b) aligning the faceplate with the recess of the golf club head;
- (c) welding the faceplate to the golf club head;
- (d) heat treating the club head assembly to a temperature just below the β-transus temperature of the α-β Ti alloy for a predetermined amount of time;
- (e) quenching the club head assembly to room temperature;
- (f) aging the club head assembly to a temperature just below the Ti3Al solution temperature;
- and
- (g) reducing the temperature of the club head assembly to room temperature by increments of at most 400° C. every hour.
5 more elements
A method of a club head assembly, the method comprising:
- (a) providing a golf club head having a recess, and providing a faceplate, wherein the golf club head and the faceplate are formed from an α-β Ti alloy, the α-β Ti alloy comprising between 6 wt % Al, 6 wt % V, and 2 wt % Sn;
- (b) aligning the faceplate with the recess of the golf club head;
- (c) welding the faceplate to the golf club head;
- (d) heat treating the club head assembly to a temperature just below the β-transus temperature of the α-β Ti alloy for a predetermined amount of time;
- (e) quenching the club head assembly to room temperature
- (f) aging the club head assembly to a temperature just below the Ti3Al solution temperature;
- and
- (g) reducing the temperature of the club head assembly to room temperature by increments of at most 400° C. every hour.
5 more elements