Method of manufacturing non-oriented electrical steel sheet
AssigneeJfe Steel Corporation
InventorsTomoyuki OKUBO, Masanori UESAKA, Yoshiaki ZAIZEN, Yoshihiko ODA
Life of this patent
Estimating the term…
Loading patent…
AssigneeJfe Steel Corporation
InventorsTomoyuki OKUBO, Masanori UESAKA, Yoshiaki ZAIZEN, Yoshihiko ODA
Estimating the term…
To stably improve the magnetic flux density by utilizing induction heating and radiant heating during final annealing of a non-oriented electrical steel sheet. A method of manufacturing a non-oriented electrical steel sheet, including subjecting a slab having a predetermined chemical composition to hot rolling with or without performing hot-rolled sheet annealing, and then to cold rolling either once, or twice or more with intermediate annealing performed therebetween, and then to final annealing, where a material before final cold rolling has a recrystallization ratio of less than 80% and a {100}<011> intensity of 8 or less in a ¼ layer, and in the final annealing, an average heating rate from 600° C. to 720° C. is 50° C./s or higher, and an average heating rate from 720° C. to 760° C. is 5° C./s or higher.
A method of manufacturing a non-oriented electrical steel sheet, comprising:
Dependencies are inferred from the claim text.