Process for making an erosion and wear resistant shot chamber for die casting application
AssigneeQingyou Han
InventorQingyou Han
Life of this patent
Estimating the term…
Abstract
A process of forming an erosion, oxidation, and wear resistant shot chamber, either a gooseneck or a shot sleeve, is provided. The process utilizes a self-healing erosive wear resistant coating on a liner of refractory metal to serve as the working surfaces of a shot chamber. Such a shot chamber is expected to have an improved service life for die casting of corrosive metals and alloys, including hot chamber die casting of aluminum alloys. An improved hot dipping process using stirring in the motel metal bath is also disclosed.
Claims20
A method for forming an erosion, oxidation, and wear resistant composite die casting shot chamber, the method comprising of the steps of:
- preparing a liner made of refractory metallic materials with melting temperatures higher than 1600° C.;
- coating the liner with a self-healing coating which has a metallurgical bond to the liner, wherein the coating is also capable of promoting the formation of a metallurgical bond between ferrous alloy and the liner in a casting process;
- placing the coated liner in a mold cavity and using it as a core for forming the working surfaces of the shot chamber;
- pouring a ferrous liquid alloy into the mold cavity to bond the coated liner with a metallurgical bond and to form a solid composite shot chamber after the liquid alloy is solidified on the coated liner;
- machining the solid composite shot chamber to its final dimensions;
- and
- covering the outside surfaces of the ferrous alloy with a conventional thick coating used in the casting industry.
A method of claim, 1 wherein the said coating on the liner is a zinc coating.
A method for forming an erosion, oxidation, and wear resistant composite shot chamber for die casting processes, the method comprising the steps of:
- preparing a refractory metal liner in the form of a tube coated with a layer of oxidation resistant coating;
- coating the outer surface of the coated refractory metal tube with a solder material;
- preparing a ferrous alloy shot chamber and heating it up to desired temperatures;
- and
- shrink fitting the shot chamber on the liner tube while the heat of the shot chamber melts the said solder material and bond the shot chamber with the liner tube.
A method for coating a solid metallic article with a layer of intermetallic compounds from a molten metallic material, the method comprising the steps of:
- preparing a solid article with clean surfaces;
- preparing a metallic bath at a temperature at least 20° C. higher than the liquidus of the material;
- submerging the solid article in a molten metallic bath;
- stiffing the molten metallic bath to enhance the chemical reaction between the material of the solid article and the molten metallic material at their interfaces;
- and
- removing the solid article out of the metallic bath after a layer of intermetallic phases have been formed on the solid article.
Dependencies are inferred from the claim text.