Substrate for flexible device and method for producing the same
AssigneeToyo Seikan Group Holdings, Ltd.
InventorsToshihiko MIYAZAKI, Hirohisa MASUDA, Hiroshi SHIMOMURA, Kouji NANBU
Life of this patent
Estimating the term…
Loading patent…
AssigneeToyo Seikan Group Holdings, Ltd.
InventorsToshihiko MIYAZAKI, Hirohisa MASUDA, Hiroshi SHIMOMURA, Kouji NANBU
Estimating the term…
A substrate for flexible device. The substrate has a nickel-plated metal sheet having a nickel-plating layer formed on at least one surface of a metal sheet or a nickel-based sheet, and a glass layer of an electrically-insulating layered bismuth-based glass on a surface of the nickel-plating layer or the nickel-based sheet. An oxide layer having a roughened surface is formed on the surface of the nickel-plating layer or the surface of the nickel-based sheet, and the bismuth-based glass contains 70 to 84% by weight of Bi2O3, 10 to 12% by weight of ZnO, and 6 to 12% by weight of B2O3. Also disclosed is a method for producing the substrate for flexible device, a substrate for an organic EL device, a sheet used as a substrate for flexible device, a method for producing the sheet and a bismuth-based lead-free glass composition.
A sheet which is used for substrate for flexible device, the sheet including either a nickel-plated metal sheet including a nickel-plating layer formed on at least one surface of a metal sheet or a nickel-based sheet, wherein a roughened oxide layer is formed on either the surface of the nickel-plating layer or the surface of the nickel-based sheet.
A method for producing a sheet which is used for substrate for flexible device, including baking in an oxygen-containing atmosphere a nickel-plated metal sheet having a nickel-plating layer formed on at least one surface of a metal sheet or a nickel-based sheet to form an oxide layer on either a surface of the nickel-plating layer or a surface of the nickel-based sheet.
A bismuth-based lead-free glass composition containing 70 to 84% by weight of Bi2O3, 10 to 12% by weight of ZnO, and 6 to 12% by weight of B2O3.