Ultrathin atomic layer deposition film accuracy thickness control
AssigneeLam Research Corporation
InventorsJun Qian, Hu Kang, Adrien LaVoie, Seiji Matsuyama, Purushottam Kumar
Life of this patent
Estimating the term…
Abstract
Methods for depositing ultrathin films by atomic layer deposition with reduced wafer-to-wafer variation are provided. Methods involve exposing the substrate to soak gases including one or more gases used during a plasma exposure operation of an atomic layer deposition cycle prior to the first atomic layer deposition cycle to heat the substrate to the deposition temperature.
Claims35
A method for depositing a silicon oxide film by atomic layer deposition on a semiconductor substrate, the method comprising:
- (a) inserting a substrate into a chamber;
- (b) after inserting the substrate into the chamber and prior to performing a first cycle of atomic layer deposition at a deposition temperature, raising the substrate's temperature to about the deposition temperature by exposing the substrate to a soak gas for a duration of about 500 seconds or less;
- and
- (c) performing the atomic layer deposition,
- wherein a cycle of the atomic layer deposition comprises
- exposing the substrate to a silicon-containing precursor in a non-plasma environment for a duration sufficient to substantially adsorb the silicon-containing precursor to the surface of the substrate and
- exposing the substrate to an oxidant in a plasma environment to form at least a portion of the silicon oxide film,
- wherein soaking the substrate comprises exposing the substrate to a soak gas comprising only one or more gases used when exposing the substrate to the oxidant in the plasma environment during the atomic layer deposition cycle to form the at least a portion of the silicon oxide film, and
- wherein the thickness of the silicon oxide film deposited by the atomic layer deposition is less than about 5 nm.
A method for depositing a film by atomic layer deposition on a semiconductor substrate, the method comprising:
- (a) inserting a substrate into a chamber;
- and
- (b) after inserting the substrate into the chamber and prior to performing a first cycle of atomic layer deposition at a deposition temperature, raising the substrate's temperature to about the deposition temperature by exposing the substrate to a soak gas for a duration of about 500 seconds or less;
- and
- (c) performing the atomic layer deposition,
- wherein a cycle of the atomic layer deposition comprises
- exposing the substrate to a precursor in a non-plasma environment for a duration sufficient to substantially adsorb the precursor to the surface of the substrate,
- exposing the substrate to a second reactant in a plasma environment to form at least a portion of the film, and
- wherein soaking the substrate comprises exposing the substrate to a soak gas comprising only one or more gases used when exposing the substrate to the second reactant in the plasma environment during the atomic layer deposition cycle to form the at least a portion of the film, and
- wherein the thickness of the film deposited by the atomic layer deposition is less than about 5 nm.
An apparatus for processing semiconductor substrates, the apparatus comprising:
- (a) one or more stations, each reaction station comprising a pedestal for holding a substrate;
- (b) at least one outlet for coupling to a vacuum;
- (c) one or more process gas inlets for coupling to precursor and reactant sources;
- (d) a robot for inserting substrates into the one or more reaction chambers;
- and
- (e) a controller for controlling operations in the apparatus, comprising machine-readable instructions for:
- (i) inserting a substrate into one of the one or more stations,
- (ii) introducing a soak gas for a duration of about 500 seconds or less;
- (iii) introducing a silicon-containing precursor for a duration sufficient to substantially adsorb the silicon-containing precursor onto the surface of the substrate;
- (iv) introducing a second reactant into the one or more reaction chambers and igniting a plasma;
- and
- (v) repeating (iii) and (iv) to form a film on the substrate, the film having a thickness less than about 5 nm,
- wherein the soak gas in (ii) comprises only one or more gases used in (iv).
Dependencies are inferred from the claim text.