Abstract
A powder bed material can include from 80 wt % to 100 wt % metal particles having a D50 particle size distribution value from 4 μm to 150 μm. From 10 wt % to 100 wt % of the metal particles can be surface-activated metal particles having in intact inner volume and an outer volume with structural defects. The structural defects can exhibit an average surface grain density of 50,000 to 5,000,000 per mm2.
Claims15
A powder bed material, comprising 80 wt % to 100 wt % metal particles having a D50 particle size distribution value from 4 μm to 150 μm, wherein 10 wt % to 100 wt % of the metal particles are surface-activated metal particles having in intact inner volume and an outer volume with structural defects, and wherein the structural defects exhibit an average surface grain density of 50,000 to 5,000,000 per mm2.
A material set, comprising:
- a powder bed material, comprising 80 wt % to 100 wt % metal particles having a D50 particle size distribution value from 4 μm to 150 μm, wherein 10 wt % to 100 wt % of the metal particles are surface-activated metal particles having in intact inner volume and an outer volume with structural defects, and wherein the structural defects exhibit an average surface grain density of 50,000 to 5,000,000 per mm2;
- and
- a binder fluid to adhere a first portion of the powder bed material relative to a second portion of the powder bed material not in contact with the fluid.
A method of three-dimensional printing, comprising:
- spreading a powder bed material to form a powder layer having a thickness of from 20 μm to 400 μm, wherein the powder bed material includes 80 wt % to 100 wt % metal particles having a D50 particle size distribution value from 4 μm to 150 μm, wherein 10 wt % to 100 wt % of the metal particles are surface-activated metal particles having in intact inner volume and an outer volume with structural defects, and wherein the structural defects exhibit an average surface grain density of 50,000 to 5,000,000 per mm2;
- selectively binding a first portion of the powder bed material to form a green layer within the powder layer;
- and
- building up additional green layers by sequentially repeating the spreading and the selectively binding of the powder bed material until a green three-dimensional object is formed.