Anisotropic expansion of silicon-dominant anodes
AssigneeEnevate Corporation
InventorsRahul Kamath, Fred Bonhomme, Ian Browne
Life of this patent
Estimating the term…
Loading patent…
AssigneeEnevate Corporation
InventorsRahul Kamath, Fred Bonhomme, Ian Browne
Estimating the term…
Systems and methods for anisotropic expansion of silicon-dominant anodes may include forming an anode by pyrolyzing an active material layer comprising a binder and silicon particles in a temperature range of 600 to 800° C.; and forming a battery cell comprising a cathode, an electrolyte, and the anode, where the anode comprises the pyrolyzed active material layer on a current collector. A lateral expansion of the anode during operation may be less than 2%, less than 1%, or less than 0.6%. The active material layer may be pyrolyzed on the current collector or may be pyrolyzed on a substrate before laminating on the current collector. The anode active material layer may be pyrolyzed using a 1 hour dwell time or less or using a 2 hour dwell time or less. The active material layer may be pyrolyzed in a temperature range of 650 to 800° C.
A method of forming a battery cell, the method comprising:
A method of forming a battery cell, the method comprising:
Dependencies are inferred from the claim text.