Method for manufacturing a three-dimensional object from a poly(arylene sulfide) polymer
AssigneeSolvay Specialty Polymers USA, LLC
InventorsRyan HAMMONDS, Lee CARVELL, Jason RICH, Stéphane JEOL, William E. SATTICH, Christopher WARD
Life of this patent
Estimating the term…
Abstract
The invention pertains to a method for manufacturing a three-dimensional (3D) object, using a powdered material (M) comprising at least one poly(arylene sulfide) polymer, in particular to a 3D object obtainable by selective sintering from this powdered polymer material (M).
Claims18
1-15. (canceled)
A method for manufacturing a three-dimensional (3D) object, comprising:
- a) depositing successive layers of a powdered material (M) comprising:
- a polymeric component (P) comprising at least one poly(arylene sulfide) polymer (PAS), having a calcium content of less than 200 ppm, as measured by X-ray Fluorescence (XRF) analysis calibrated with standards of known calcium content as determined by Inductively Coupled Plasma Optical Emission Spectrometry (ICP-OES) according to ASTM UOP714-07, and
- from 0.01 to 10 wt. % of at least one flow agent (F), based on the total weight of the material (M),
- b) selectively sintering each layer prior to deposition of the subsequent layer.
A powdered material (M) for additive manufacturing, comprising:
- one polymeric component (P) comprising at least one poly(arylene sulfide) polymer (PAS), having a calcium content of less than 200 ppm, as measured by Inductively Coupled Plasma Optical Emission Spectrometry (ICP-OES) according to ASTM UOP714-07, and
- from 0.01 to 10 wt. % of at least one flow agent (F), based on the total weight of the material (M).
A three-dimensional (3D) object obtainable by laser sintering from a powdered material (M), comprising:
- one polymeric component (P) comprising at least one poly(arylene sulfide) polymer (PAS), having a calcium content of less than 200 ppm, as measured by X-ray Fluorescence (XRF) analysis calibrated with standards of known calcium content as determined by Inductively Coupled Plasma Optical Emission Spectrometry (ICP-OES) according to ASTM UOP714-07, and
- from 0.01 to 10 wt. % of at least one flow agent (F), based on the total weight of the material (M).
A method for manufacturing a three-dimensional (3D) object, the method comprising using a powdered material (M) comprising:
- one polymeric component (P) comprising at least one poly(arylene sulfide) polymer (PAS), having a calcium content of less than 200 ppm, as measured by X-ray Fluorescence (XRF) analysis calibrated with standards of known calcium content as determined by Inductively Coupled Plasma Optical Emission Spectrometry (ICP-OES) according to ASTM UOP714-07, and
- from 0.01 to 10 wt. % of at least one flow agent (F), based on the total weight of the material (M).
- to manufacture of a three-dimensional (3D) object using additive manufacturing.
A method for manufacturing a powdered material (M), the method comprising using a polymeric component (P) comprising at least one poly(arylene sulfide) polymer (PAS), having a calcium content of less than 200 ppm, as measured by X-ray Fluorescence (XRF) analysis calibrated with standards of known calcium content as determined by Inductively Coupled Plasma Optical Emission Spectrometry (ICP-OES) according to ASTM UOP714-07, and from 0.01 to 10 wt. % of at least one flow agent (F), based on the total weight of the material (M),
- for the manufacture of a powdered material (M) for additive manufacturing.
Dependencies are inferred from the claim text.