US 2021/0171722 A1Published application
Controlling the rheology of a metal ore residue
AssigneeCoatex
InventorsMehdi BOUZID, Christian JACQUEMET, Benoit MAGNY, Jacques MONGOIN
Life of this patent
Estimating the term…
Abstract
A method can prepare an aqueous mineral suspension from an aqueous metal ore residue into which there is introduced a polymer (P) having a molecular weight Mw measured by GPC of from 100,000 to 3.106 g/mol and prepared by free radical polymerization of at least one anionic monomer (m). The suspension produced may have a Brookfield viscosity greater than 2,000 mPa·s and/or a flow threshold of greater than 40 Pa.
Claims18
A method for preparing:
- the method comprising:
- adding, in an aqueous metal ore residue, a first component comprising a polymer (P) with a molecular mass Mw, measured by GPC, in a range of from 100,000 to 3·106 g/mol and prepared by a method comprising radical polymerization at a temperature greater than 50° C., the polymer (P) comprising:
- a polymer (P1) prepared in direct emulsion from reagents comprising (a) an anionic monomer comprising a polymerizable olefinic unsaturation and a carboxylic acid group;
- and (b) an ester of acrylic acid and/or methacrylic acid, in the presence of a radical-generating compound comprising ammonium persulfate and/or, an alkaline metal persulfate and optionally further an —FeII, FeIII, CuI, and/or CuII ion;
- and/or
- a polymer (P2) prepared in reverse emulsion from reagents comprising (a) an anionic monomer comprising a polymerizable olefinic unsaturation and a carboxylic acid group, optionally as a salt;
- and (c) acrylamide, an acrylamide derivative, and/or a salt of an acrylamide derivative, in the presence of a radical-generating compound comprising ammonium persulfate and/or an alkaline metal persulfate and optionally further an comprising FeII, FeIII, CuI, and/or CuII ion,
- wherein the aqueous mineral suspension produced has (i) a dry solids content greater than 40 wt. % of the suspension and
- (ii-a) a Brookfield viscosity, measured at 100 rpm and at 25° C., greater than 2,000 mPa·s;
- (ii-b) a flow threshold measured at a temperature of 25° C. using a rheometer with imposed shearing, equipped with a bladed spindle, for a particular torsional loading, greater than 40 Pa, and/or
- (ii-c) a Brookfield viscosity, measured at 100 rpm and at 25° C., greater than 2,000 mPa·s and a flow threshold, measured at a temperature of 25° C. using a rheometer with imposed shearing, equipped with a bladed spindle, for a particular torsional loading, greater than 40 Pa.
8 more elements
An aqueous mineral suspension,
- comprising:
- an aqueous metal ore residue;
- and
- a polymer (P) with a molecular mass Mw, measured by GPC, ranging from 100,000 to 3·106 g/mol and prepared by a method comprising radical polymerization at a temperature greater than 50° C., and the polymer (P) comprising:
- polymer (P1) prepared in direct emulsion from reagents comprising an anionic monomer comprising a polymerizable olefinic unsaturation and a carboxylic acid group;
- and (b) ester of acrylic acid and/or methacrylic acid, in the presence of a radical-generating compound comprising ammonium persulfate and/or alkaline metal persulfate and optionally further an FeII, FeIII, CuI, and/or CuII ion;
- a polymer (P2) prepared in reverse emulsion from comprising (a) an anionic monomer comprising a polymerizable olefinic unsaturation and a carboxylic acid group, optionally as a salt;
- and (c) acrylamide, an acrylamide derivative, and/or a salt of an acrylamide derivative;
- in the presence of a radical-generating compound comprising ammonium persulfate and/or alkaline metal persulfate and optionally further an FeII, FeIII, CuI, and/or CuII ion,
- wherein the aqueous mineral suspension, has (i) a dry solids content greater than 40 wt. % of the suspension and:
- (ii-a) a Brookfield viscosity, measured at 100 rpm and at 25° C., greater than 2,000 mPa·s;
- (ii-b) a flow threshold measured at a temperature of 25° C. using a rheometer with imposed shearing, equipped with a bladed spindle, for a particular torsional loading, greater than 40 Pa;
- and
- (ii-c) a Brookfield viscosity, measured at 100 rpm and at 25° C., greater than 2,000 mPa·s and a flow threshold, measured at a temperature of 25° C. using a rheometer with imposed shearing, equipped with a bladed spindle, for a particular torsional loading, greater than 40 Pa.
11 more elements