Cathode materials for lithium ion batteries
AssigneeSaft America
InventorsXilin CHEN, Saori TOKUOKA, Frank CAO, Jian DONG, Carine MARGEZ, Owen OU, Thomas GRESZLER
Life of this patent
Estimating the term…
Loading patent…
AssigneeSaft America
InventorsXilin CHEN, Saori TOKUOKA, Frank CAO, Jian DONG, Carine MARGEZ, Owen OU, Thomas GRESZLER
Estimating the term…
Provided is a positive electrode active material for a lithium-ion battery, the positive electrode active material including a blend of a doped lithium manganese iron phosphate (dLMFP) according to the formula: LiMnxFeyM1−x−yPO4, wherein 0.9<x+y<1; and M is one or more selected from the group consisting of Mg, Ca and Ba with one or both of a lithium nickel cobalt manganese oxide (NMC) compound having a Ni content greater than 0.6 relative to a total amount of metals other than Li and a lithium nickel cobalt aluminum oxide (NCA) compound. In particular, provided is a blend at a weight ratio of dLMFP to NMC and/or NCA (i.e., dLMFP:(NMC+NCA)) of >70:<30, such as 75:25, 80:20, 85:15, 90:10, etc.
A positive electrode active material for use in a lithium-ion secondary battery, the positive electrode active material comprising a blend of a doped lithium manganese iron phosphate (dLMFP) compound according to the following formula (1) with one or both of a lithium nickel manganese cobalt oxide (NMC) compound according to the following formula (2) or a lithium nickel cobalt aluminum (NCA) compound according to the following formula (3):
A positive electrode active material for use in a lithium-ion secondary battery, the positive electrode active material comprising a blend of a doped lithium manganese iron phosphate (dLMFP) compound according to the following formula (1) with a lithium nickel manganese cobalt oxide (NMC) compound according to the following formula (2):
A positive electrode active material for use in a lithium-ion secondary battery, the positive electrode active material comprising a blend of a doped lithium manganese iron phosphate (dLMFP) compound according to the following formula (1) with a lithium nickel cobalt aluminum (NCA) compound according to the following formula (3):
Dependencies are inferred from the claim text.