Back to results
US 2021/0083056 A1Published application
Semiconductor Device with Implant and Method of Manufacturing Same
AssigneeTaiwan Semiconductor Manufacturing Company, Ltd.
InventorsYu-Chang Lin, Tien-Shun Chang, Chun-Feng Nieh, Huicheng Chang
Life of this patent
Estimating the term…
Abstract
A FinFET is provided including a channel region containing a constituent element and excess atoms, the constituent element belonging to a group of the periodic table of elements, wherein said excess atoms are nitrogen, or belong to said group of the periodic table of elements, and a concentration of said excess atoms in the channel region is in the range between about 1019 cm−3 and about 1020 cm−3.
Claims20
A device comprising:
- a transistor having a channel region, the channel region containing a constituent element and excess atoms, the constituent element belonging to a group of the periodic table of elements, wherein
- said excess atoms are nitrogen, or belong to said group of the periodic table of elements, and
- a concentration of said excess atoms in the channel region is in the range between about 1019 cm−3 and about 1021 cm−3;
- and
- an isolation region adjacent the transistor, the isolation region also containing said excess atoms at a concentration in a range between about 1020 cm−3 and about 1021 cm−3.
2 more elements
A device comprising:
- a gate, wherein an upper width of the gate is larger than a lower width of the gate by a value exceeding about 1 nanometer,
- a channel region containing a constituent element and excess atoms, the constituent element belonging to a group of the periodic table of elements, wherein said excess atoms are nitrogen, or belong to said group of the periodic table of elements, and
- a concentration of said excess atoms in the channel region is in the range between about 1019 cm−3 and about 1021 cm−3.
12-20. (canceled)
A device comprising:
- a transistor having a channel region, the channel region containing a constituent element and excess atoms, the constituent being an elemental group-IV or compound group-IV semiconductor, wherein
- said excess atoms are selected from the group consisting of Ge, carbon, and nitrogen, with a concentration of said excess atoms in the channel region being in the range between about 1019 cm−3 and about 1021 cm−3;
- a gate over the channel region, an upper width of the gate being larger than a lower width of the gate by at least 1 nanometer;
- and
- an isolation region adjacent the transistor, the isolation region also containing said excess atoms at a concentration in a range between about 1020 cm−3 and about 1021 cm−3.
2 more elements