Microfibrous cellulose-containing substance
AssigneeOji Holdings Corporation
InventorsGo BANZASHI, Hiroyuki NAGATANI, Shino IWAI
Life of this patent
Estimating the term…
Abstract
A microfibrous cellulose aggregate containing microfibrous cellulose having an average fiber width of 2 nm to 50 nm and a liquid compound including at least one of water or an organic solvent. The content of the microfibrous cellulose is from 6 mass % to 80 mass % per the mass of the entire microfibrous cellulose aggregate, and the content of the liquid compound is at least 15 mass % per the mass of the entire microfibrous cellulose aggregate.
Claims9
A method for manufacturing a microfibrous cellulose-containing substance, the method comprising:
- concentrating a first microfibrous cellulose dispersion liquid containing microfibrous cellulose having fibers with an average fiber width of 2 nm to 200 nm and a first dispersion medium wherein a surface charge of the microfibrous cellulose is positive,
- wherein the concentrating comprises flocculating the microfibrous cellulose contained in the first microfibrous cellulose dispersion liquid, and removing the first dispersion medium by filtering the first microfibrous cellulose dispersion liquid after the flocculating;
- wherein the microfibrous cellulose is flocculated by adding one selected from the group consisting of an alkali, sodium oleate, potassium oleate, sodium laurate, sodium dodecylbenzene sulfonate, sodium alkylnaphthalene sulfonate, sodium dialkyl sulfosuccinate, sodium polyoxyethylene alkyl ether sulfate, sodium polyoxyethlyene alkyl allyl ether sulfate, sodium polyoxyethylene dialkyl sulfate, polyoxyethylene alkyl ether phosphoric acid ester, polyoxyethylene alkyl allyl ether phosphoric acid ester, carboxymethylcellulose, carboxymethyl starch, and sodium alginate to the first microfibrous cellulose dispersion liquid.
A microfibrous cellulose-containing substance, comprising:
- microfibrous cellulose having fibers with an average fiber width of 2 nm to 50 nm;
- a first liquid compound comprising at least one of water or an organic solvent;
- and
- one selected from the group consisting of an alkali, sodium oleate, potassium oleate, sodium laurate, sodium dodecylbenzene sulfonate, sodium alkylnaphthalene sulfonate, sodium dialkyl sulfosuccinate, sodium polyoxyethylene alkyl ether sulfate, sodium polyoxyethlyene alkyl allyl ether sulfate, sodium polyoxyethylene dialkyl sulfate, polyoxyethylene alkyl ether phosphoric acid ester, polyoxyethylene alkyl allyl ether phosphoric acid ester, carboxymethylcellulose, carboxymethyl starch, and sodium alginate;
- wherein a surface charge of the microfibrous cellulose is positive,
- a content of the microfibrous cellulose is from 6 mass % to 80 mass % per a mass of an entire microfibrous cellulose-containing substance;
- and
- a content of the first liquid compound is at least 15 mass % per the mass of the entire microfibrous cellulose-containing substance.
A method for remanufacturing a microfibrous cellulose dispersion liquid, the method comprising;
- concentrating a first microfibrous cellulose dispersion liquid containing microfibrous cellulose having fibers with an average fiber width of 2 nm to 200 nm and a first dispersion medium;
- and
- preparing a second microfibrous cellulose-containing solution by adding a second dispersion medium to the microfibrous cellulose concentrate obtained by the concentrating, and performing dispersion treatment on the second microfibrous cellulose-containing solution,
- wherein a surface charge of the microfibrous cellulose is positive, and
- in the preparing or the performing dispersion treatment, the second microfibrous cellulose-containing solution is adjusted to a pH of between 4 and 7 by adding an acid.