Ultrathin glass with special chamfer shape and high strength
AssigneeSCHOTT Glass Technologies (Suzhou) Co. Ltd.
InventorsNing DA, Feng HE
Life of this patent
Estimating the term…
Abstract
A chemically toughened glass article is provided that has a thickness (t) of equal to or less than 0.4 mm, a first surface, a second surface, and a compressive stress region that is defined by a compressive stress (CS) of at least 100 MPa and at least one edge connecting the first surface and the second surface. The at least one edge has at least one chamfer with a chamfer width (A) and a chamfer height (B). The chamfer has a ratio of chamfer width/chamfer height (A/B) of between 1.5-20 and the chamfer has a ratio of chamfer width/glass thickness (A/t) of at least 0.5.
Claims21
A chemically toughened glass article, comprising:
- a thickness (t) of equal to or less than 0.4 mm;
- a first surface;
- a second surface;
- a compressive stress region defined by a compressive stress (CS) of at least 100 MPa, and
- an edge connecting the first surface and the second surface,
- wherein the edge has a chamfer with a chamfer width (A) and a chamfer height (B),
- wherein the chamfer has a first ratio of chamfer width to chamfer height (A/B) of between 1.5 to 20, and
- wherein the chamfer has a second ratio of chamfer width to glass thickness (A/t) of at least 0.5.
The article of claim 12, wherein the bending strength (BS) is greater than 1200 MPa.
Dependencies are inferred from the claim text.