Process for the manufacture of enriched phospholipid compositions
AssigneeAcasti Pharma Inc.
InventorsPierre LEMIEUX, Simon DESPINS, Sarya AZIZ, Remi LABRECQUE, Nicolas BISSUEL
Life of this patent
Estimating the term…
Abstract
It is provided a process for generating enriched phospholipid compositions from raw krill oil, where such processes may be batchwise, continuous, of include both batchwise steps and continuous steps. The present technology provides high quality enriched phospholipid compositions from such methods. Moreover, the continuous process provides a significantly higher throughput compared to a batch process while concurrently providing products of equal or greater quality.
Claims24
1:
- A process for producing an enriched phospholipid composition comprising the steps of:
- mixing a raw krill oil (RKO) with an organic solvent comprising at least about 85% by weight of a C3-C8 ketone providing a RKO-containing mixture containing an aqueous portion;
- and
- fractionating the RKO-containing mixture into a first low density layer and a first higher density phospholipid-containing layer (PCL) and separating the first PCL from the first low density layer producing the enriched phospholipid composition.
2:
- The process of claim 1, further comprising
- separating the first PCL from the first low density layer producing a first separated PCL;
- mixing the first separated PCL with the organic solvent producing a PCL containing mixture;
- fractionating the PCL containing mixture into a second low density layer and a second PCL;
- and
- separating the second PCL from the second low density layer producing the enriched phospholipid composition.
3:
- A process for producing an enriched phospholipid composition comprising the steps of:
- mixing a raw krill oil (RKO) with an organic solvent comprising at least about 85% by weight of a C3-C8 ketone providing a RKO-containing mixture containing an aqueous portion;
- fractionating the RKO-containing mixture into a first low density layer and a first higher density phospholipid-containing layer (PCL);
- separating the first PCL from the first low density layer producing a first separated PCL;
- mixing the first separated PCL with the organic solvent producing a PCL containing mixture;
- fractionating the PCL containing mixture into a second low density layer and a second PCL;
- and
- separating the second PCL from the second low density layer producing the enriched phospholipid composition.
4:
- The process of claim 1, further comprising filtering the RKO-containing mixture prior to the fractionating of the RKO-containing mixture.
5:
- A process for producing an enriched phospholipid composition comprising the steps of:
- mixing a raw krill oil (RKO) with an organic solvent comprising at least about 85% by weight of a C3-C8 ketone providing a RKO-containing mixture containing an aqueous portion;
- and
- mixing the RKO-containing mixture with water and fractionating the RKO-containing mixture and water into a first low density layer and a first higher density phospholipid-containing layer (PCL) and separating the first PCL from the first low density layer producing the enriched phospholipid composition.
6:
- The process of claim 2, further comprising combining the second PCL with a stabilizing agent, a viscosity-reducing agent, or a combination thereof.
7:
- The process of claim 1, wherein the aqueous portion is substantially free of salts.
8:
- The process of claim 1, wherein the aqueous portion is substantially free of carbonate salts, bicarbonate salts, or a combination thereof.
9:
- The process of claim 1, wherein the process comprises mixing at least 100 kg RKO with the organic solvent.
10:
- The process of claim 1, wherein the process comprises mixing the RKO and the organic solvent at a ratio of about 5 to about 15 in units of volume organic solvent:kg RKO.
11:
- The process of claim 1, wherein prior to mixing the RKO and the organic solvent, the process comprises heating the RKO to a temperature from about 30° C. to about 70° C.
(canceled)
13:
- The process of claim 1, wherein the mixing of raw krill oil (RKO) with the organic solvent is performed to provide the RKO-containing mixture at a temperature of about 15° C. to about 40° C.
(canceled)
15:
- The process of claim 1, wherein the RKO-containing mixture is filtered through a first filter and a second filter.
16:
- The process of claim 1, wherein the first filter is a 10 μm filter and the second filter is a 0.45 μm filter.
17:
- The process of claim 1, wherein the RKO-containing mixture is filtered by centrifugation or decantation.
18:
- The process of claim 2, wherein the process further comprises mixing the RKO containing mixture with water at a ratio of the RKO containing mixture versus water and the aqueous portion of about 0.15 to about 0.40 in units of volume aqueous portion:kg RKO.
19:
- The process of claims 1, wherein the first separated PCL is mixed with the organic solvent at a volume ratio of about 2 to about 10.
20:
- process of claim 2, wherein the second PCL is combined with a viscosity-reducing agent comprising a volume ratio of viscosity-reducing agent to second PCL of about 0.1 to about 0.3.
21:
- The process of claim 2, wherein the stabilizing agent comprises Vitamin E.
22-23. (canceled)
24:
- The process of claim 1, wherein the enriched phospholipid composition comprises at least 75% on a dry weight basis of phospholipids.
(canceled)
Dependencies are inferred from the claim text.