Back to results
US 2021/0071277 A1Published application
Steel sheet with excellent bake hardening properties and plating adhesion and manufacturing method therefor
AssigneePosco
InventorsSang-Ho HAN, Je-Woong LEE
Life of this patent
Estimating the term…
Abstract
Provided is a steel sheet used as a material for an automotive exterior panel, etc., and a method for manufacturing the same. More particularly, provided is a cold-rolled steel sheet and a hot-dip galvanized steel sheet, which have excellent bake hardening properties, plating adhesion, and anti-aging properties, and a method of manufacturing the same.
Claims12
A steel sheet having excellent bake hardening and plating adhesion, comprising:
- in weight %, 0.005 to 0.08% of carbon (C), 1.3 to 2.3% of manganese (Mn), 0.03% or less (excluding 0%) of phosphorus (P), 0.01% or less (excluding 0%) of sulfur (S), 0.01% or less (excluding 0%) of nitrogen (N), 0.01 to 0.06% of aluminum (sol.Al), 1.0% or less (excluding 0%) of chromium (Cr), 0.1% or less (excluding 0%) of antimony (Sb), at least one selected from the group consisting of silicon (Si):
- 0.3% or less (excluding 0%), molybdenum (Mo):
- 0.2% or less (excluding 0%) and boron (B):
- 0.003% or less (excluding 0%), a remainder of iron (Fe), and unavoidable impurities, and
- as a microstructure, in area %, 1 to 5% of martensite and remaining ferrite,
- wherein a relationship (Cgb/Cf) between an Sb average area occupancy ratio (Cgb, %) of grain boundaries of a martensite phase and a ferrite phase and an average Sb area occupancy ratio (Cf, %) in a ferrite phase within 1 μm around the martensite phase, determined by the following relationship 1, at a point of ¼t in a thickness direction of the steel sheet (where t denotes a thickness (mm) of a cold rolled steel sheet is 3.5 or more,
- Cgb/Cf≥3.5 [Relationship 1]
- (where Cgb (%) indicates an Sb average area occupancy ratio of grain boundaries of a martensitic phase and a ferrite phase at a point of ¼t of a cold rolled steel sheet, and Cf (%) indicates an average Sb area occupancy ratio of a ferrite phase within 1 μm around the martensite phase).
5 more elements
A method of manufacturing a steel sheet having excellent bake hardening and plating adhesion, comprising:
- reheating a slab including, in weight %, 0.005 to 0.08% of carbon (C), 1.3 to 2.3% of manganese (Mn), 0.03% or less (excluding 0%) of phosphorus (P), 0.01% or less (excluding 0%) of sulfur (S), 0.01% or less (excluding 0%) of nitrogen (N), 0.01 to 0.06% of aluminum (sol.Al), 1.0% or less (excluding 0%) of chromium (Cr), 0.1% or less (excluding 0%) of antimony (Sb), at least one selected from the group consisting of silicon (Si):
- 0.3% or less (excluding 0%), molybdenum (Mo):
- 0.2% or less (excluding 0%) and boron (B):
- 0.003% or less (excluding 0%), a remainder of iron (Fe), and unavoidable impurities;
- hot rolling the reheated slab at a temperature in a range of 850 to 1150° C. to obtain a hot rolled steel sheet;
- cooling the hot rolled steel sheet to a temperature range of 550 to 750° C. at an average cooling rate of 10 to 70° C./sec;
- coiling the cooled hot rolled steel sheet at a temperature in a range of 550 to 750° C.;
- cold rolling the hot rolled steel sheet to obtain a cold rolled steel sheet;
- continuously annealing the cold rolled steel sheet under a hydrogen concentration of 3 to 30% by volume at a temperature in a range of Ac1+20° C. to Ac3−20° C.;
- and
- primary cooling the continuously annealed cold rolled steel sheet to 630 to 670° C. at an average cooling rate of 2 to 10° C./sec.
8 more elements
Dependencies are inferred from the claim text.