Catalytic hydrocarbon dehydrogenation
AssigneeSaudi Arabian Oil Company
InventorsMohammed Abdulmajeed Al-Daous, Hussam A. Bahlouli
Life of this patent
Estimating the term…
Abstract
A catalyst for dehydrogenation of hydrocarbons includes a support including zirconium oxide and Linde type L zeolite (L-zeolite). A concentration of the zirconium oxide in the catalyst is in a range of from 0.1 weight percent (wt. %) to 20 wt. %. The catalyst includes from 5 wt. % to 15 wt. % of an alkali metal or alkaline earth metal. The catalyst includes from 0.1 wt. % to 10 wt. % of tin. The catalyst includes from 0.1 wt. % to 8 wt. % of a platinum group metal. The alkali metal or alkaline earth metal, tin, and platinum group metal are disposed on the support.
Claims20
A catalyst for dehydrogenation of hydrocarbons, the catalyst comprising:
- a support comprising zirconium oxide and Linde type L zeolite (L-zeolite), wherein a concentration of the zirconium oxide in the catalyst is in a range of from 0.1 weight percent (wt. %) to 20 wt. %;
- from 5 wt. % to 15 wt. % of an alkali metal or alkaline earth metal, the alkali metal or alkaline earth metal disposed on the support;
- from 0.1 wt. % to 10 wt. % of tin, the tin disposed on the support;
- and
- from 0.1 wt. % to 8 wt. % of a platinum group metal, the platinum group metal disposed on the support.
A method of dehydrogenating hydrocarbons, the method comprising:
- subjecting hydrocarbons to be dehydrogenated to an operating temperature in a range of from about 500 degrees Celsius (° C.) to about 800° C. within a reactor, wherein the hydrocarbons to be hydrogenated comprise n-pentane;
- subjecting the hydrocarbons to be dehydrogenated to an operating pressure in a range of from about 0.01 bar to about 10 bar within the reactor;
- while subjecting the hydrocarbons to be dehydrogenated to the operating temperature and operating pressure within the reactor,
- introducing a diluent gas to the hydrocarbons to be dehydrogenated, the diluent gas comprising hydrogen and inert gas;
- and
- using a catalyst disposed within the reactor to dehydrogenate the hydrocarbons to be dehydrogenated in the presence of the diluent gas within the reactor, the catalyst comprising:
- a support comprising zirconium oxide and L-zeolite, wherein a concentration of the zirconium oxide in the catalyst is in a range of from 0.1 weight percent (wt. %) to 20 wt. %;
- from 5 wt. % to 15 wt. % of an alkali metal or alkaline earth metal, the alkali metal or alkaline earth metal disposed on the support;
- from 0.1 wt. % to 10 wt. % of tin, the tin disposed on the support;
- and
- from 0.1 wt. % to 8 wt. % of a platinum group metal, the platinum group metal disposed on the support, wherein the catalyst forms catalyst grains of about 200 micrometers (μm) to about 500 μm in size.
A method of preparing a catalyst for dehydrogenation of hydrocarbons, the method comprising:
- mixing a Linde type L zeolite (L-zeolite) with an aqueous solution of a first additive to form a first slurry, the first additive comprising a salt or complex comprising zirconium;
- drying the first slurry in the presence of oxygen to form a first solid;
- mixing the first solid with an aqueous solution of a second additive to form a second slurry, the second additive comprising a salt comprising an alkali metal or an alkaline earth metal;
- drying the second slurry to form a second solid;
- mixing the second solid with an ethanolic solution of a third additive to form a third slurry, the third additive comprising a salt or complex comprising tin;
- drying the third slurry to form a third solid;
- mixing the third solid with an aqueous solution of a fourth additive to form a fourth slurry, the fourth additive comprising a salt or complex comprising a platinum group metal;
- drying the fourth slurry in the presence of oxygen to form the catalyst having a composition comprising:
- from 0.1 weight percent (wt. %) to 20 wt. % of zirconium derived from the first additive;
- from 5 wt. % to 15 wt. % of the alkali metal or alkaline earth metal derived from the second additive;
- from 0.1 wt. % to 10 wt. % of the tin derived from the third additive;
- from 0.1 wt. % to 8 wt. % of the platinum group metal derived from the fourth additive;
- and
- a balance of L-zeolite.
Dependencies are inferred from the claim text.