Molecular sieve/fiber composite material and preparation method thereof
AssigneeZhejiang University
InventorsJie Fan, Lisha Yu, Liping Xiao, Hao Chen, Xiaoqiang Shang
Life of this patent
Estimating the term…
Loading patent…
AssigneeZhejiang University
InventorsJie Fan, Lisha Yu, Liping Xiao, Hao Chen, Xiaoqiang Shang
Estimating the term…
The disclosure provides a molecular sieve/fiber composite material comprising molecular sieves and a fiber, the molecular sieves are distributed on the fiber surface and directly contact the fiber surface; the particle diameter D90 of the molecular sieves is 0.01 to 50 μm, the particle size D50 of the molecular sieves is 0.005 to 25 μm; the molecular sieves are distributed uniformly on the fiber surface of the fiber. The disclosure also provides a preparation method for the molecular sieve/fiber composite material and various applications. The molecular sieve/fiber composite material has high strength, elastic recovery ability, and dimensional stability, making the composite material strong and durable. The molecular sieve/fiber composite material has a simple structure, low cost, strong stability, high repeatability of performance, and high practical efficiency, and provides the application in the fields of hemostasis, beauty, deodorization, sterilization, water purification, air purification, and radiation resistance.
A molecular sieve/fiber composite material comprising molecular sieves and a fiber, the molecular sieves are distributed on the fiber surface and directly contact the fiber surface;
24-82. (canceled)
Dependencies are inferred from the claim text.