Fluorine rubber composition and crosslinked fluorine rubber product
AssigneesDaikin Industries, Ltd., Bridgestone Corporation
InventorsMasashi ARAI, Daisuke OHTA, Akinori UEDA, Yasuhiro ODA, Junichi ORIDE
Life of this patent
Estimating the term…
Abstract
A fluoroelastomer composition, and a crosslinked fluoroelastomer obtained by crosslinking the fluoroelastomer composition. The fluoroelastomer composition contains 10 to 60 parts by mass of a carbon black (B) and 0.1 to 10 parts by mass of a peroxide cross-linking agent (C) per 100 parts by mass of a peroxide-crosslinkable fluoroelastomer (A). The carbon black (B) has a number of foreign particles of 30/mm2 or less measured as described herein.
Claims7
A fluoroelastomer composition comprising 10 to 60 parts by mass of a carbon black (B) and 0.1 to 10 parts by mass of a peroxide cross-linking agent (C) per 100 parts by mass of a peroxide-crosslinkable fluoroelastomer (A), wherein
- the carbon black (B) has a number of foreign particles measured under the following measurement conditions of 30/mm2 or less,
- Measurement conditions:
- A dispersion is prepared by dispersing the carbon black (B) in ethanol such that a content of the carbon black (B) is 0.1% by mass, 1 ml of the dispersion is collected, the collected dispersion is vacuum-filtered with a filter, a residue of the carbon black (B) captured on a surface of the filter is observed with a scanning electron microscope, and the number of foreign particles having an aspect ratio of 1.1 or less and a Heywood diameter of 5 μm or more is measured.
A crosslinked fluoroelastomer obtained by peroxide-crosslinking a fluoroelastomer composition comprising a peroxide-crosslinkable fluoroelastomer (A), a carbon black (B), and a peroxide cross-linking agent (C), wherein
- the crosslinked fluoroelastomer has a hardness at 25° C. of 60 to 90, and
- a number of foreign particles having an aspect ratio of 1.1 or less and a Heywood diameter of 5 μm or more present on a fracture surface obtained by tensile fracture of the crosslinked fluoroelastomer at 170° C. is 25/mm2 or less.
Dependencies are inferred from the claim text.