Method for degreasing shaped ceramic molded body and method for manufacturing ceramic fired body
AssigneeNGK Insulators, Ltd.
InventorTetsuya ONOGI
Life of this patent
Estimating the term…
Abstract
A ceramic molded body including a ceramic powder and an organic binder includes an oxidizable ceramic powder as the ceramic powder, includes an oxidizable metal or metal compound, or is in contact with a solid body including an oxidizable metal or metal compound. In a hydrogen atmosphere, the ceramic molded body is heated to a maximum temperature set within a range of 1,100° C. to 1,400° C. at a heating rate of more than 25° C./h, is degreased at the maximum temperature, and is then cooled at a cooling rate of more than 25° C./h.
Claims12
A method for degreasing a ceramic molded body, comprising degreasing a ceramic molded body including a ceramic powder and an organic binder,
- wherein the ceramic molded body includes an oxidizable ceramic powder as the ceramic powder, includes an oxidizable metal or metal compound, or is in contact with a solid body including an oxidizable metal or metal compound, and
- in an atmosphere of hydrogen gas alone or in an atmosphere of a mixture of an inert gas and hydrogen gas with a hydrogen gas concentration of 20% by volume or more, the ceramic molded body is heated to a maximum temperature set within a range of 1,100° C. to 1,400° C. at a heating rate of more than 25° C./h, is degreased at the maximum temperature, and is then cooled at a cooling rate of more than 25° C./h.
A method for degreasing a ceramic molded body, comprising degreasing a ceramic molded body including a ceramic powder and an organic binder,
- wherein the ceramic molded body includes an oxidizable ceramic powder as the ceramic powder, includes an oxidizable metal or metal compound, or is in contact with a solid body including an oxidizable metal or metal compound, and
- in an atmosphere of hydrogen gas alone or in an atmosphere of a mixture of an inert gas and hydrogen gas with a hydrogen gas concentration of 20% by volume or more, the ceramic molded body is heated to an intermediate temperature set within a range of 600° C. to 1,100° C. at a heating rate of more than 25° C./h, is held at the intermediate temperature for a predetermined period of time, is heated to a maximum temperature set above the intermediate temperature within a range of 1,100° C. to 1,400° C. at a heating rate of more than 25° C./h, is degreased at the maximum temperature, and is then cooled at a cooling rate of more than 25° C./h.
Dependencies are inferred from the claim text.