A thermoformable biaxially oriented coextruded polyester film comprising a copolyester base layer B, a first polyester outer layer A1 and a second polyester outer layer A2, wherein said outer layers are disposed on opposite surfaces of said base layer, and wherein: (i) said base layer B comprises a copolyester derived from terephthalic acid (TA) and a second aromatic dicarboxylic acid and one or more diol(s), wherein said second aromatic dicarboxylic acid is present in the copolyester in an amount of from about to 5 about 20 mol % of the acid fraction of the copolyester; (ii) the polyester of each of said outer layers A1 and A2 is selected from polyethylene terephthalate (PET); and (iii) the thickness of the base layer constitutes at least 90% of the total thickness of the coextruded multi-layer polyester film.
A thermoformable biaxially oriented coextruded polyester film comprising a copolyester base layer B, a first polyester outer layer A1 and a second polyester outer layer A2, wherein said outer layers are disposed on opposite surfaces of said base layer, and wherein:
A film according to any preceding claim wherein said second aromatic dicarboxylic acid is isophthalic acid (IPA).
A film according to any preceding claim wherein said copolyester of said base layer exhibits a crystalline melting point (Tm) in the range of 210 to 240° C. and which is at least 10° C. lower than the crystalline melting point of said outer layer polyester, and/or a glass transition temperature (Tg) in the range of 60 to 90° C.
A film according to any preceding claim wherein the total thickness of the film is from about 50 to about 350 μm.
A film according to any preceding claim wherein the film exhibits a shrinkage at 150° C. of no more than 3.0% in each of the machine and transverse dimensions of the film;
A film according to any preceding claim which exhibits a haze of no more than 3.0% and/or a total light transmission (TLT) of at least 85%.
A film according to any preceding claim wherein the base layer does not contain a particulate filler, and preferably wherein the outer layers do not contain a particulate filler.
A film according to any preceding claim wherein the coextruded film exhibits an Ultimate Tensile Strength (UTS) in each of the longitudinal and transverse directions of the film of at least 10.0 kgf/mm2 , and/or an Elongation To Break (ETB) in each of the longitudinal and transverse directions of the film of at least 150%, and/or an F5 value (stress at 5% elongation) in each of the longitudinal and transverse directions of the film of at least 8.0 kgf/mm2 .
A film according to any preceding claim wherein a functional layer is disposed on one or both of the outer layer(s) (A1 and/or A2) of the coextruded polyester film, wherein said functional layer is selected from adhesion-promoting layers and ink-receptive layers.
A film according to any preceding claim wherein the film is thermoformable at a temperature in the range of 130° C. to 200° C., preferably at least about 135° C., preferably at least 140° C., preferably at least about 150° C., preferably from about 150° C. to about 195° C., preferably 160° C. to 190° C., more preferably 160° C. to 180° C.
A film according to any preceding claim wherein the copolyester base layer exhibits a degree of crystallinity which is lower than that of either of the outer layers, preferably wherein [(XC-OUTER)-(XC-BASE)/(XC-OUTER)×100] is at least 40%, preferably at least 45%, preferably no more than 70%, preferably no more than 60%, preferably no more than 55%, preferably no more than 50%, wherein XC-BASE is the degree of crystallinity of the copolyester base layer and XC-OUTER is the degree of crystallinity of the outer layers, and wherein the degree of crystallinity of a layer is calculated from the enthalpy of fusion measured by Differential Scanning Calorimetry.
A film according to any preceding claim wherein the degree of crystallinity (XC-OUTER) of each of the outer layers is, independently, in the range of from 25% to 50%, and/or the degree of crystallinity (XC-BASE) of the copolyester base layer is in the range of from 10% to 20%, wherein the degree of crystallinity of a layer is calculated from the enthalpy of fusion measured by Differential Scanning Calorimetry.
An electronic device comprising a touch-screen interface wherein the external surface of said touch-screen interface is a thermoformed biaxially oriented coextruded polyester film comprising a copolyester base layer B, a first polyester outer layer A1 and a second polyester outer layer A2, wherein said outer layers are disposed on opposite surfaces of said base layer, and wherein:
Use of a biaxially oriented coextruded polyester film comprising a copolyester base layer B, a first polyester outer layer A1 and a second polyester outer layer A2, wherein said outer layers are disposed directly on opposite surfaces of said base layer, and wherein:
A method of manufacture of an electronic device comprising a touch-screen interface, said method comprising the steps of:
A process according to claim 31 or 32 wherein heat-setting is conducted in a multiple-zone crystalliser wherein the temperature of the final zone is lower than the temperature of the first zone, preferably wherein the first zone is at a temperature of from about 205 to about 215° C., and the final zone is at a temperature preferably in the range of from about 170 to about 190° C.