Photocatalyst nanocomposite
AssigneeImam Abdulrahman Bin Faisal University
InventorsNuhad Abdullah ALOMAIR, Hanan Hussein Amin Mohamed
Life of this patent
Estimating the term…
Abstract
An efficient photocatalyst nanocomposite comprising reduced graphene oxide, noble metal, and a metal oxide prepared by a one-step method that utilizes date seed extract as a reducing and nanoparticle determining size agent. The photocatalyst of the invention is a more effective sunlight photocatalyst than that prepared by traditional method in the photo decomposition of organic compounds in contaminated water.
Claims19
A photocatalyst nanocomposite, comprising:
- noble metal nanoparticles, metal oxide nanoparticles, and reduced graphene oxide (rGO),
- wherein the photocatalyst nanocomposite comprises rGO in an amount in the range of 40 wt. % to 60 wt. % of the total weight of the photocatalyst nanocomposite,
- wherein the noble metal nanoparticles have a diameter in the range of 5 nm to 50 nm and are dispersed on the metal oxide nanoparticles which are present on the rGO;
- the metal oxide nanoparticles have a diameter in the range of 20 nm to 80 nm;
- and the noble metal nanoparticles are present in an amount in the range of 2 mol. % to 10 mol. % based on the molar amount of the metal oxide nanoparticles;
- and
- wherein the metal oxide nanoparticles comprise a metal oxide of at least one metal selected from the group consisting of Sc, Ti, V, Cr, Mn, Fe, Co, Ni, Zn, Y, Zr, Nb, and Mo.
A photocatalyst nanocomposite, comprising:
- gold nanoparticles,
- ZnO nanoparticles, and
- reduced graphene oxide (rGO),
- wherein the photocatalyst nanocomposite comprises the rGO in an amount in the range of 45 wt. % to 55 wt. % of the total weight of the photocatalyst nanocomposite;
- wherein the gold nanoparticles have a diameter in the range of 10 nm to 30 nm;
- wherein the gold nanoparticles are dispersed on hexagonal wurtzite ZnO nanoparticles having diameter in the range of 20 nm to 60 nm;
- and
- wherein the gold nanoparticles are present in an amount in the range of 2 mol. % to 10 mol. % based on the molar amount of the zinc oxide nanoparticles.
A method of preparing a composition comprising noble metal nanoparticles, comprising:
- preparing an aqueous solution or suspension comprising a noble metal precursor,
- mixing the aqueous suspension with date seed extract to form a mixture, and
- heating the mixture at temperature in the range of 100-200° C. for a time in the range of 10 to 20 hours;
- wherein the date seed extract is prepared by grinding date seed and heating the ground date seed in water at a temperature in the range of 60 to 100° C. for a time in the range of 1 to 5 hours, and separating solids to form the date seed extract in the form of a liquid, and the noble metal nanoparticles have a diameter in the range of 5 nm to 30 nm.
Dependencies are inferred from the claim text.