Abstract
A process of producing an extinguishing agent includes dissolving 5 g to 90 g of diammonium hydrogen phosphate, 0.1 g to 60 g of urea, 1 g to 90 g of ammonium carbonate, 5 g to 90 of ammonium sulfate, and 20 g to 250 g of potassium carbonate in 400 ml to 550 ml of water at a temperature of 30° C. to 90° C. to form a first solution; mixing the first solution with 5 g to 500 g of surfactant to undergo a first reaction for forming a second solution; and mixing the second solution with 1000 ml of water to undergo a second reaction for forming an extinguishing agent.
Claims4
A process of producing an extinguishing agent, comprising the steps of:
- (a) dissolving 5 g to 90 g of diammonium hydrogen phosphate, 0.1 g to 60 g of urea, 1 g to 90 g of ammonium carbonate, 5 g to 90 of ammonium sulfate, and 20 g to 250 g of potassium carbonate in 400 ml to 550 ml of water at a temperature of 30° C. to 90° C. to form a first solution;
- (b) mixing the first solution with 5 g to 500 g of surfactant to undergo a first reaction for forming a second solution;
- and
- (c) mixing the second solution with 1000 ml of water to undergo a second reaction for forming an extinguishing agent.