Back to results
US 2020/0347476 A1Published application
High-strength steel sheet having excellent processability and method for manufacturing same
AssigneePosco
InventorsYeon-Sang AHN, Chang-Hyo SEO, Kang-Hyun CHOI, Eul-Yong CHOI
Life of this patent
Estimating the term…
Abstract
Provided is a high-strength steel sheet having a tensile strength of 780 MPa or higher. The high-strength steel sheet has a low yield ratio and excellent ductility (El) and strain hardening exponent (n) and thus has enhanced processability.
Claims11
A high strength steel sheet having excellent workability, comprising:
- in weight %, 0.06 to 0.18% of carbon (C), 1.5% or less (excluding 0%) of silicon (Si), 1.7 to 2.5% of manganese (Mn), 0.15% or less (excluding 0%) of molybdenum (Mo), 1.0% or less (excluding 0%) of chromium (Cr), 0.1% or less of phosphorus (P), 0.01% or less of sulfur (S), 1.0% or less (excluding 0%) of aluminum (Al), 0.001 to 0.04% of titanium (Ti), 0.001 to 0.04% of niobium (Nb), 0.01% or less of nitrogen (N), 0.01% or less (excluding 0%) of boron (B), 0.05% or less (excluding 0%) of antimony (Sb), and a remainder of Fe and other inevitable impurities, and
- as a microstructure, ferrite having an area fraction of 40% or more and bainite, fresh martensite, and retained austenite as a remainder,
- wherein a ratio (Mb/Mt) of a total fraction (Mt) of the fresh martensite and a fraction (Mb) of fresh martensite adjacent to the bainite is 60% or more, and a ratio (Ms/Mt) of the total fraction (Mt) of the fresh martensite and a fraction (Ms) of fine fresh martensite having an average particle size of 3 μm or less is 60% or more.
A method of manufacturing a high strength steel sheet having excellent workability, the method comprising:
- reheating, at a temperature in a range of 1050 to 1300° C., a steel slab including, in weight %, 0.06 to 0.18% of carbon (C), 1.5% or less (excluding 0%) of silicon (Si), 1.7 to 2.5% of manganese (Mn), 0.15% or less (excluding 0%) of molybdenum (Mo), 1.0% or less (excluding 0%) of chromium (Cr), 0.1% or less of phosphorus (P), 0.01% or less of sulfur (S), 1.0% or less (excluding 0%) of aluminum (Al), 0.001 to 0.04% of titanium (Ti), 0.001 to 0.04% of niobium (Nb), 0.01% or less of nitrogen (N), 0.01% or less (excluding 0%) of boron (B), 0.05% or less (excluding 0%) of antimony (Sb), a remainder of Fe and other inevitable impurities;
- preparing a hot-rolled steel sheet by finishing hot-rolling the reheated steel slab at an Ar3 transformation point or higher;
- coiling the hot rolled steel sheet in a temperature range of 400 to 700° C.;
- after the coiling, primary cooling at a cooling rate of 0.1° C./s or less to room temperature;
- after the cooling, producing a cold rolled steel sheet by cold rolling at a cold reduction ratio of 40 to 70%;
- continuously annealing the cold rolled steel sheet in a temperature range of Ac1+30° C. to Ac3−20° C.;
- after the continuously annealing, performing a secondary cooling at a cooling rate of 10° C./s or less (excluding 0° C./s) to 630 to 670° C.;
- after the secondary cooling, performing a third cooling to 400 to 500° C. at a cooling rate of 5° C./s or more in a hydrogen cooling facility;
- maintaining for 70 seconds or more after the third cooling;
- hot-dip galvanizing after the maintaining;
- and
- after the hot-dip galvanizing, performing a final cooling to Ms or less at a cooling rate of 1° C./s or more.
9 more elements
Dependencies are inferred from the claim text.