The present invention provides a ferritic stainless steel sheet and a method for manufacturing the same. A ferritic stainless steel sheet has a composition containing C: 0.001 to 0.020%, Si: 0.05 to 0.35%, Mn: 0.05 to 1.00%, P: 0.04% or less, S: 0.01% or less, Al: 0.001 to 0.300%, Cr: 10.0 to 13.0%, Ni: 0.75 to 1.50%, Ti: 0.05 to 0.35%, and N: 0.001 to 0.020%, with the balance being Fe and inevitable impurities, in which γI [AD] represented by formula (1) below is 65% or more, and a metal structure has an average crystal grain size of 45 μm or less: γI [%]=24Ni+12Mn+6Cu−18Si−12Cr−12Mo+188 (1), where Ni, Mn, Cu, Si, Cr, and Mo represent contents of the respective elements (percent by mass), and an element not contained represents 0.
A ferritic stainless steel sheet having a composition containing, in percent by mass,
Dependencies are inferred from the claim text.