High-strength steel having excellent low-yield-ratio characteristics, and manufacturing method therefor
AssigneePosco
InventorHwan-Gyo Jung
Life of this patent
Estimating the term…
Abstract
A high-strength steel having excellent low-yield-ratio characteristics, according to one embodiment of the present invention, comprises, by wt %, 0.06-0.12% of C, 0.2-0.5% of Si, 1.5-2.0% of Mn, 0.003-0.05% of Al, 0.01% or less of N, 0.02% or less of P, 0.003% or less of S, 0.05-0.5% of Cr, 0.05-0.5% of Mo, 0.01-0.05% of Nb, 0.0005-0.005% of Ca and the balance of Fe and other inevitable impurities, and comprises polygonal ferrite as a microstructure, wherein the area fraction of the polygonal ferrite is 10-30% and the average hardness of the polygonal ferrite can be 180 Hv or less.
Claims16
A high-strength steel material having an excellent low yield ratio characteristic, the steel material comprising, by wt %:
- 0.06 to 0.12% of C, 0.2 to 0.5% of Si, 1.5 to 2.0% of Mn, 0.003 to 0.05% of Al, 0.01% or less of N, 0.02% or less of P, 0.003% of less of S, 0.05 to 0.5% of Cr, 0.05 to 0.5% of Mo, 0.01 to 0.05% of Nb, and 0.0005 to 0.005% of Ca, with a balance of Fe and other unavoidable impurities, and
- polygonal ferrite as a microstructure,
- wherein the polygonal ferrite has an area fraction of 10 to 30% and an average hardness of 180 Hv or less.
A method of manufacturing a high-strength steel material having an excellent low yield ratio characteristic, the method comprising:
- reheating a slab including, by wt %:
- 0.06 to 0.12% of C, 0.2 to 0.5% of Si, 1.5 to 2.0% of Mn, 0.003 to 0.05% of Al, 0.01% or less of N, 0.02% or less of P, 0.003% or less of S, 0.05 to 0.5% of Cr, 0.05 to 0.5% of Mo, 0.01 to 0.05% of Nb, and 0.0005 to 0.005% of Ca, with a balance of Fe and other unavoidable impurities at a temperature range of 1100 to 1160° C.;
- roughly rolling the reheated slab at an end temperature of 1050° C. or higher;
- starting finish rolling of the roughly rolled slab in a temperature range of 980° C. or lower and ending the finish rolling in a temperature range of (Ar3+50° C.) to 900° C.;
- first cooling the finish-rolled steel material down to a temperature range of (Ar3−40° C.) to (Ar3−70° C.) at a first cooling rate;
- and
- second cooling the first cooled steel material down to a temperature range of 350 to 400° C. at a second cooling rate.