Back to results
US 2020/0346981 A1Published application
Composition Having Plasma-treated Recycled Steel Fibers
AssigneeIntegrated Composite Construction Systems, LLC
InventorDOUGLAS DARLING
Life of this patent
Estimating the term…
Abstract
The invention relates to a composition having plasma-treated recycled steel fibers within the matrix.
Claims9
1-25. (canceled)
A jersey barrier, comprising:
- a component made according to the process of claim 27,
- wherein the dimensions of the component comprise a height of 850-900 mm with a 40 mm wide lip overhanging 120-125 mm on a street side, said lip joins a trunk section at a 110 degree angle, and a top surface and bottom surface of the component are flat, and parallel to one another, said top surface having an width of 270-280 mm, with said lip comprising 120-125 mm and a top remaining section of the trunk comprising 150-155 mm, said component having a footer 75-90 mm thick, said footer on one side meets the trunk at a 90 degree angle, and on the street side the footer meets the trunk at on offset angle of 135 degrees by having a sloped portion that is 120-140 mm in height, said component having a length from 850-4000 mm, and said component having a plurality of steel rebars forming a matrix that is disposed within an interior of the component, said matrix connected to rebar mounting posts extending from the bottom surface of the footer, said rebar mounting posts extend 75-90 mm beyond the bottom surface of the component, said component having a plurality of tensioning cables disposed within the interior of the component, said tensioning cables comprising heat cured cables cured to 40,000 psi.
A method of producing a component, comprising the steps:
- (i) cleaning recycled steel macrofibers,
- wherein said macrofibers are of lengths between about 18 to about 38 mm and in diameters between about 0.38 to about 0.63 mm,
- wherein the recycled steel macrofibers are cleaned by plasma treatment to remove organic contamination, remove surface oxides, increase surface hydrophilic property, and improve adhesion,
- wherein the plasma treatment is selected from the group consisting of:
- Argon plasma micro-sandblasting, Hydrogen plasma treatment for removal of surface oxides on the recycled steel fibers, Helium plasma treatment, Nitrogen plasma treatment, and Oxygen plasma treatment;
- (ii) surface-modifying the recycled steel macrofibers using plasma enhanced chemical vapor deposition to coat the recycled steel macrofibers with one or more layers selected from the group consisting of:
- carbon, silicon, carbon nanotubes, silicon carbide, silicon nitride, and mixtures thereof;
- (iii) surface energy modifying the recycled steel macrofibers using plasma treatment to have one or more ultra-thin layers of a film that adjusts wetting properties to improve of the wettability and increase the mixability of the macrofibers in a cement composition;
- (iv) mixing first constituents comprising:
- cement of Blaine fineness of about 280 to about 360 m2/kg;
- sand, wherein said sand is provided at a mass ratio of about 0.75 to about 1.25 of said cement;
- silica fume, wherein said silica fume is provided at a mass ratio of about 0.15 to about 0.4 of said cement;
- silica flour, wherein said silica flour is provided at a mass ratio of about 0.15 to about 0.3 of said cement;
- microinclusions, wherein said microinclusions are provided at a mass ratio of up to about 0.35 of said cement, and
- wherein said mixing results in a first homogeneous mix;
- (v) mixing second constituents comprising:
- at least one high-range water-reducing admixture;
- and
- water,
- wherein said water is provided at a mass ratio of about 0.2 to about 0.35 of said cement, and
- wherein said mixing of said second constituents results in a second homogenous mix;
- (vi) mixing said first homogeneous mix with said second homogeneous mix to form a uniform cement-containing paste;
- (vii) blending the recycled steel macrofibers into said uniform cement-containing paste,
- wherein said macrofibers are provided at a mass ratio of up to about 0.35 of said cement,
- wherein said recycled steel macrofibers are blended until distributed approximately uniformly in the resultant cement-containing paste;
- (viii) forming said resultant cement-containing paste in the shape of said component, wherein said forming is done by techniques selected from the group consisting of:
- spin casting, extrusion molding, pressure molding, pouring into forms, and combinations thereof;
- and
- (ix) curing said component by placing in an environment of approximately 100% relative humidity for about seven days at ambient temperature, then submersing in water of approximately 85° C. to about 91° C. for about three to about five days, and then heating in air at approximately 85° C. to about 91° C. for about one to about two days.
26 more elements