Titanium Alloy For Medical Devices
AssigneeMiRus LLC
InventorNoah Roth
Life of this patent
Estimating the term…
Abstract
A medical device at least partially formed of a novel titanium alloy of at least about 90 wt. % of a solid solution of titanium and molybdenum.
Claims20
A medical device at least partially formed of a metal alloy, said metal alloy includes at least about 90 wt. % of a solid solution of titanium, molybdenum, and optionally additional metal additive, said metal alloy includes at least 51 wt. % titanium, 0.1-40 wt. % molybdenum, and up to 5 wt. % of said additional metal additive.
A method of manufacturing a medical device at least partially formed of a metal alloy having a cross sectional thickness of less than 15 mm comprising:
- a. forming a member from a metal alloy that forms at least a portion of said medical device, said metal alloy formed by a hot or cold press process and has been optionally annealed and optionally aged, said member optionally having a cylindrical shape, said metal alloy including at least about 90 wt. % of a solid solution of titanium and molybdenum, said metal alloy optionally having a yield strength of 170-230 ksi, said metal alloy optionally including carbon and oxygen and having a carbon to oxygen atomic ratio of at least about 2.5:1;
- said metal alloy optionally having a carbon to nitrogen atomic ratio of less than about 40:1, said metal alloy optionally having an oxygen to nitrogen atomic ratio of less than about 30:1, said metal alloy optionally having an average grain size of at least 5 ASTM, said metal alloy optionally having an elongation of at least 8%, said metal alloy having a hardness of 340-600 HV.
A method of manufacturing a medical device at least partially formed of a metal alloy having a cross-sectional thickness of less than 15 mm comprising:
- a. rod member of a titanium alloy, said rod member having an average cross-sectional thickness of greater than 15 mm, said titanium alloy including at least about 95 wt. % of a solid solution of titanium and molybdenum, said titanium alloy a) having a yield strength of at least 170 ksi, b) including carbon and oxygen wherein a oxygen atomic ratio is at least about 2.5:1, c) including carbon, oxygen, and nitrogen and having a carbon to nitrogen atomic ratio of less than about 40:1 and an oxygen to nitrogen atomic ratio of less than about 30:1, d) having an average grain size of over 5 ASTM, e) having an elongation of said member of at least 8%;
- and/or f) having a hardness of at least 340 Hv;
- and
- b. forming said titanium alloy into at least a portion of said medical device and reducing said average cross-sectional thickness of said titanium alloy to less than 15 mm, wherein said titanium alloy is optionally age treated at a temperature of 300-800° C. for at least 10 minutes;
- wherein said titanium alloy is optionally cold rolled to a 5-90% reduction without subjecting said titanium alloy to a solution treatment;
- and,
- wherein said rod member is optionally reduced in cross-sectional thickness by at least 40% per ASTM E8.
Dependencies are inferred from the claim text.