Ternary zinc-nickel-iron alloys and alkaline electrolytes or plating such alloys
AssigneeMacDermid, Incorporated
InventorsGeorge Bokisa, Tony Oriti, Markus Jahn
Life of this patent
Estimating the term…
Abstract
A ternary zinc-nickel-iron alloy and aqueous alkaline electrolyte for electroplating the alloy includes zinc, nickel, and a complex of an iron salt.
Claims19
An aqueous alkaline electroplating bath for depositing a ternary zinc-nickel-iron alloy on a substrate, the aqueous alkaline electroplating bath comprising zinc ions, nickel ions, and iron ions, wherein the iron ions are provided in the aqueous alkaline electroplating bath as a complex of a water soluble iron salt and an iron complexing agent.
An aqueous alkaline zinc-nickel-iron electroplating bath, comprising:
- about 4 grams per liter to about 50 grams per liter of zinc;
- about 0.1 grams per liter to about 10 grams per liter nickel;
- about 0.1 gram per liter to about 10 grams per liter iron;
- about 50 grams per liter to about 220 grams per liter of an alkaline compound effective to provide the bath with a pH more than about 13;
- and
- about 2 g/l to about 200 g/l of a nickel complexing agent;
- wherein the iron is provided in the aqueous alkaline electroplating bath as a complex of a water soluble iron salt and an iron complexing agent.
The aqueous alkaline electroplating bath of claim 15, wherein the brightener comprises at least one of N-methylpyridinium-3-carboxylate or salt thereof (trigonelline), 1-benzylnicotinate, or sulfopropylpyridinium. Claims 17-28 (Cancelled)
An electrical connector comprising:
- an aluminum substrate,
- a zinc-nickel-iron ternary alloy electroplated on the substrate, the zinc-nickel-iron ternary alloy including, by weight, about 7% to about 16% nickel, about 0.5% to about 8% iron, and balance zinc, and
- a passivate provided on the zinc-nickel-iron ternary alloy electroplate.
Dependencies are inferred from the claim text.