Back to results
US 2019/0369325 A1Published application
High chlorine content low attenuation optical fiber
AssigneeCorning Incorporated
InventorsGeorge Edward Berkey, Dana Craig Bookbinder, Ming-Jun Li, Pushkar Tandon
Life of this patent
Estimating the term…
Abstract
An optical fiber having a core comprising silica and greater than 1.5 wt % chlorine and less than 0.5 wt % F, said core having a refractive index Δ1MAX, and an inner cladding region having refractive index Δ2MIN surrounding the core, where Δ1MAX>Δ2MIN.
Claims14
A method for making an optical fiber preform, the method comprising:
- exposing a silica soot core preform having a surface area greater than 10 m2/gm to an atmosphere comprising a chlorine-containing compound at temperatures higher than 1300° C. to form a chlorine doped soot core preform;
- and
- sintering the soot core preform to form a core portion of the optical fiber preform such that the chlorine concentration in said core portion is greater than or equal to 1.5 wt % chlorine.
A method for making a single mode optical fiber, the method comprising:
- depositing, via a PCVD (plasma chemical vapor deposition) process, a core glass layer inside a glass tube which is comprised of SiO2, the glass layer comprising chlorine doped silica having greater than 3 wt % Cl;
- and
- collapsing the tube to eliminate the open centerline and thereby forming an optical fiber preform.